Search found 2 matches

by Mary Price
Fri Mar 29, 2013 5:28 pm
Forum: Techniques and Tools
Topic: I need help with a difficult slump
Replies: 3
Views: 6349

Re: I need help with a difficult slump

Thanks Marty, I'll give that a try.
by Mary Price
Fri Mar 29, 2013 4:57 pm
Forum: Techniques and Tools
Topic: I need help with a difficult slump
Replies: 3
Views: 6349

I need help with a difficult slump

I am attempting to make a vase, which is made with System 96 glass. It is put together as follows: a clear circle for the center, then each of the petals is placed on the outside edge of the circle over lapping by about 1.5 inches. The petals also over lap a bit. I then place a second clear circle o...