Re: Brand New Kiln Question

A brand new kiln, how exciting! The batt or kiln wash will protect the kiln floor from spills. You also need to paint it on any shelves you use to stop the glass from sticking. For the shelves you can also use thin fire shelf paper or fiber paper, available from kiln suppliers. If there's no sun, he...