I want to buy a circle cutter. I've never used one but it seems the Silbertschnitt (6 wheel) & Fletcher-Terry(3wheel) are good ones. I read a carbide head is available for the Fletcher is that true of the Silbertschnitt also.
Thank you,
Chris
Search found 13 matches
- Tue Mar 22, 2016 3:27 pm
- Forum: Techniques and Tools
- Topic: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
- Replies: 12
- Views: 24511
- Thu Mar 20, 2014 8:20 am
- Forum: Techniques and Tools
- Topic: Papyros, Kiln Liner and Bullseye Thinfire papers
- Replies: 5
- Views: 11941
Re: Papyros, Kiln Liner and Bullseye Thinfire papers
I have used thin fire (old & new) and switched to Papyros. I don't have a shrinkage or split problem, do have very nice backs. I use BE glass.
- Sun Mar 16, 2014 10:01 pm
- Forum: Techniques and Tools
- Topic: Borax and firepolish after haze/devit?
- Replies: 4
- Views: 7290
Re: Borax and firepolish after haze/devit?
Stephen>> Some of the pieces were composed of black and deep royal blue. One piece all 1114 blue. A third piece was 1114 and 4223 on this one only the 1114 had the hazy splotches. I clean carefully and keep my fingers off. I hope this makes more sense
- Sun Mar 16, 2014 1:35 am
- Forum: Techniques and Tools
- Topic: Borax and firepolish after haze/devit?
- Replies: 4
- Views: 7290
Re: Borax and firepolish after haze/devit?
I meant to say the haze on the black glass gives the black the appearance that it has a light coating of bronze on the top.
- Sat Mar 15, 2014 11:38 am
- Forum: Techniques and Tools
- Topic: Borax and firepolish after haze/devit?
- Replies: 4
- Views: 7290
Borax and firepolish after haze/devit?
This is the first time I have ever had haze/devit (re my post on haze & fire schedule). BE 1114 has a goodly amount the black haze almost makes it looks like it has bronze hue.
Will making up the borax mix or buying the superspray and firepolishing take care of the devit?
Chris
Will making up the borax mix or buying the superspray and firepolishing take care of the devit?
Chris
- Sat Mar 15, 2014 11:34 am
- Forum: Techniques and Tools
- Topic: haze (devit?) on glass what is wrong with schedule
- Replies: 5
- Views: 7910
Re: haze (devit?) schedules clarified
Marty - I am firing on mullite shelf that is washed with HotFire and I used Papyros (which I have been using successfully in my smaller kilns. I meant for my schedule to be 2 columns but they merged so here are the schedules I used for the first and second firing. The devit is mainly on the BE Blue ...
- Sat Mar 15, 2014 2:19 am
- Forum: Techniques and Tools
- Topic: haze (devit?) on glass what is wrong with schedule
- Replies: 5
- Views: 7910
Re: haze (devit?) on glass what is wrong with schedule
Drat it is late and I hit the wrong key before I finished typing. In reading the board I also noticed several people anneal by going Full to 960, the 100 to 800 and last 200 to 700. Why the last two steps instead of one. First fireing 2nd firing Ramp / dph/ hold 300 - 500 - 2 300 - 500 - 2 500 - 115...
- Sat Mar 15, 2014 2:13 am
- Forum: Techniques and Tools
- Topic: haze (devit?) on glass what is wrong with schedule
- Replies: 5
- Views: 7910
haze (devit?) on glass what is wrong with schedule
I've used two schedules (the second one I slowed down on) but still having hazing problems - actually the second schedule gave me more haze on all my Bullseye transparent deep royal #1114.
First schedule 2nd fireing
300 - 500dph -2min
First schedule 2nd fireing
300 - 500dph -2min
- Mon Mar 03, 2014 6:03 pm
- Forum: Techniques and Tools
- Topic: schedule help? Oval 39" with side & top elements
- Replies: 0
- Views: 20870
schedule help? Oval 39" with side & top elements
I need some schedule help/advice, please. All my kilns are JenKen - the old kiln is a 16" fiber Bonnie Glo with side elements, my new oval 24x39 has side & top elements. I am attaching a pic of my first fire - all bulleye 2 layers. The 10.5 square was perfect as was the 6" retro square...
- Fri Feb 14, 2014 8:49 pm
- Forum: Techniques and Tools
- Topic: BE vs Hotline Hifire ?
- Replies: 2
- Views: 6277
Re: BE vs Hotline Hifire ?
Thank you - I appreciate all the detailed comparisions.
Chris
Chris
- Fri Feb 14, 2014 2:32 am
- Forum: Techniques and Tools
- Topic: Jen-Ken Kilns
- Replies: 6
- Views: 27164
Re: Jen-Ken Kilns
I just (a few days ago) got my 5th Jen Ken. I have 2 brick(AF3p, one with bead door) and 2 fiber (Bonnie Glo) and now the Oval 13.
JenKen is a great company - the support is terrific and the kiln quality is excellent.
Chris
JenKen is a great company - the support is terrific and the kiln quality is excellent.
Chris
- Fri Feb 14, 2014 2:28 am
- Forum: Techniques and Tools
- Topic: BE vs Hotline Hifire ?
- Replies: 2
- Views: 6277
BE vs Hotline Hifire ?
What is the difference in the back of the glass fired on hotline hi fire vs Bullseye vs Papyros? I have been using papyros( switched from TF becuase easier to clean up) in my small kiln and Primo Primer (it gives a very smooth back) on my molds. I want to omit the papyros if I can get a smooth back....
- Sun Feb 24, 2013 7:47 am
- Forum: Techniques and Tools
- Topic: Fuse Master Wave form slumping mold - more holes?
- Replies: 1
- Views: 5275
Fuse Master Wave form slumping mold - more holes?
I recently purchased the infinity series (texture plate and wave form slumping mold) from fuse master. There is only one hole at the bottom of the bowl form. Does it need more holes? Has anyone used this/drilled holes. Any tips?