Effetre 104coe Bullseye 90 coe rods
I have been using Bullseye glass for beads recently. I wanted to combine some torchwork items with fused Bullseye pieces. I was not diligent enough in keeping BE and Effetre rods completely separate. I recently have some beads that cracked, and when trying to figure out which rod was the culprit, I ...
- Sat Sep 08, 2012 1:23 pm
- Forum: Techniques and Tools
- Topic: Do you have fusing and annealing temps for 104 coe
- Replies: 1
- Views: 4757
Do you have fusing and annealing temps for 104 coe
I have lost my notes for firing Effetre soft glass.
I would like to try something with rods and murrini, but do not remember the full fuse temp, or best annealing tempurature.
Has anyone here done fusing with this mainly bead making glass?
I would like to try something with rods and murrini, but do not remember the full fuse temp, or best annealing tempurature.
Has anyone here done fusing with this mainly bead making glass?