Suppliers??



Sorry, I didn't know I had posted to the wrong discussion page. I have deleted and will now ask again.

Does anyone know where to purchase laser cut dichroic pieces like butterflies, or swirls? I think Pacific Art Glass sells them, any other suggestions? :?

Thanks!

Casey
by caseyalb
Mon Jun 02, 2003 11:15 am
Forum: Techniques and Tools
Topic: Grit on face of fused pieces
Replies: 5
Views: 10442

Thanks Lynda. That sounds like a good idea too. I do have access to a compressor so I will try that. :D
by caseyalb
Mon Jun 02, 2003 8:42 am
Forum: Techniques and Tools
Topic: Grit on face of fused pieces
Replies: 5
Views: 10442

Thank you both for the information. I have been very careful with closing the kiln and keeping it brushed/vacuumed and it seems to be helping. If this does not work I will look into the cement. It doesn't seem that the top has any damage to it but you never know. Thanks again!
by caseyalb
Tue May 27, 2003 3:41 pm
Forum: Techniques and Tools
Topic: Grit on face of fused pieces
Replies: 5
Views: 10442

Grit on face of fused pieces

I have recently purchased a top loading kiln. I noticed this weekend that it seems to be getting grit or tiny pieces of fire brick on top of my work. I have brushed the top and gone over it with a vacuum to remove any loose particles. Does anyone have any other solutions?