RE-slumping
Hello all, I just peeked into my kiln at a beautiful 14" bowl and noticed that one of the edges has a scalloped raised edge. The kiln is at 600 and coming down. It already annealed for two hours. I'm not going to like this ripple. Can I just start now and go ahead and run it through the slumpin...
- Sat Jan 17, 2015 12:14 am
- Forum: Techniques and Tools
- Topic: Tiny hole
- Replies: 4
- Views: 7598
Re: Tiny hole
I can not ever post a picture. For an unknown reason. But I filled the tiny hole with matching fine frit and added a similare design element. It was successful and place in the CoOp Gallery for sale.
- Sat Jan 10, 2015 4:34 pm
- Forum: Techniques and Tools
- Topic: Tiny hole
- Replies: 4
- Views: 7598
Tiny hole
Argh, gorgeous piece. 15 x 15". Perfect, other that a very tiny hole. Any suggestions on repairing and re fusing. The hole is 1/8" x 1/4". This piece is a high low surface. It is a cracked glass piece that is two layers but on a single layer section it has small dot enhancements and t...
- Fri Dec 19, 2014 1:19 pm
- Forum: Techniques and Tools
- Topic: Sharpie paint pens
- Replies: 5
- Views: 8058
Re: Sharpie paint pens
I used the gold after I fired the piece
- Fri Dec 19, 2014 1:19 pm
- Forum: Techniques and Tools
- Topic: Sharpie paint pens
- Replies: 5
- Views: 8058
Re: Sharpie paint pens
I used the gold after I fired the piece
- Wed Dec 17, 2014 1:13 am
- Forum: Techniques and Tools
- Topic: woven strips of glass--name?
- Replies: 3
- Views: 5391
Re: woven strips of glass--name?
My woven platters sell in the co op gallery that I belong to for 225. 00 for a 12" square. It is a great product to sell
- Wed Dec 17, 2014 1:11 am
- Forum: Techniques and Tools
- Topic: Sharpie paint pens
- Replies: 5
- Views: 8058
Re: Sharpie paint pens
Yes. I love them. The Oil Based ones. I made 35 Red Cardinals and offered people personal names on them. They came out beautifully. I used the extra fine point
- Wed Dec 10, 2014 2:16 pm
- Forum: Techniques and Tools
- Topic: Odd crack
- Replies: 6
- Views: 7596
Re: Odd crack
I think your correct and this happenned on a piece a while back. It actually had a large crack on the top layer with soft edges. Very cool looking actually, I put it in my gallery and it actually sold quickly! For this piece I did go faster, I began at 450 dph and that is a schedule I use for small ...
- Mon Dec 08, 2014 8:36 pm
- Forum: Techniques and Tools
- Topic: Odd crack
- Replies: 6
- Views: 7596
Re: Odd crack
I have been trying to upload a pic. How do I do that. Help
- Mon Dec 08, 2014 7:53 pm
- Forum: Techniques and Tools
- Topic: Odd crack
- Replies: 6
- Views: 7596
Odd crack
There is a crack that is only on the top layer of my 14" platter. It is healed and soft. Not through the second layer. It also did not crack through the design on the piece. Why would this occur. It is. Small squiggle shape. Not n S or a c shape. It appears that it cracked and then fused togeth...
- Thu Nov 20, 2014 11:41 pm
- Forum: Techniques and Tools
- Topic: Thermocouple
- Replies: 17
- Views: 19135
Re: Thermocouple
It was the most frustrating experience.we have been at this for a month and could not get it solved. Thankful we got to the bottom of it.
- Thu Nov 20, 2014 12:53 am
- Forum: Techniques and Tools
- Topic: Thermocouple
- Replies: 17
- Views: 19135
Re: Thermocouple
POST MORTEM So, all of the little parts replace, down to the wires, literally and my kiln lid still would not heat past 880. It ramped perfectly to 600 but by 700 it slowed down to a few degrees per hour. I eventually got some help from Bartlett, wonderful technician that worked with me troubleshoot...
- Thu Nov 20, 2014 12:44 am
- Forum: Techniques and Tools
- Topic: Wall elements
- Replies: 3
- Views: 5080
Re: Wall elements
Thank you. I will have my new lid in a couple of days, whew! In the mean time I attempted to fuse a small 9" plate with a poinsettia in the center...I went with an adjusted schedule, a full fuse, but ramped slowly, 175dph. I still got little bubbles. They when I formed it I got thermal shock. O...
- Sat Nov 15, 2014 12:31 am
- Forum: Techniques and Tools
- Topic: Wall elements
- Replies: 3
- Views: 5080
Wall elements
I am curious to know what the difference is between using the side elements or the lid. My Olympic Kiln is equipped with both. Although I always use the lid. This is a 186GFELTC and the largest kiln that uses 120, so this kiln can not use both at the same time. Either lid or wall. Is there any reaso...
- Thu Nov 13, 2014 4:14 am
- Forum: Techniques and Tools
- Topic: grinder or cutting system?
- Replies: 4
- Views: 6456
Re: grinder or cutting system?
Regardless you should have both, develop a well equipped shop with all tools of convenience. I know master glass artists that use grinders and saws and cutting systems. Glass sometimes has a mind of its own regardless of your skill, glass will do what it wants
- Wed Nov 12, 2014 2:02 am
- Forum: Techniques and Tools
- Topic: grinder or cutting system?
- Replies: 4
- Views: 6456
Re: grinder or cutting system?
Well I would start with a good cutting system. You can cold work a rough edge by hand with a stone or a diamond dremmel tool. I have the Beetle bits system and love it.
- Mon Nov 10, 2014 1:41 pm
- Forum: Techniques and Tools
- Topic: Thermocouple
- Replies: 17
- Views: 19135
Re: Thermocouple
Well I now have a new TC, Relay switches, elements and lid, all is well with my world. Happy glass melting to all
- Mon Nov 10, 2014 2:38 am
- Forum: Techniques and Tools
- Topic: Thermocouple
- Replies: 17
- Views: 19135
Re: Thermocouple
Thank you Bert, I have it all running now. There was a fried wire that connects to one of the elements. My husband is going to be replaceing those wires in th next few days. I need to catch up on a few orders first. Right now I am having some good firing with the body elements. I did not know that y...
- Sun Nov 09, 2014 3:23 am
- Forum: Techniques and Tools
- Topic: Thermocouple
- Replies: 17
- Views: 19135
Re: Thermocouple
Update. This kiln is fitted with wall elements. This model lets you choose which to use, lid or wall. I never use the wall, but I just now fired them up and VIOLA they are working. I am at 900 and rising. So perhaps my voltage is ok after all and the issue with the lid wiring. I wonder still how wil...
- Sun Nov 09, 2014 3:01 am
- Forum: Techniques and Tools
- Topic: Thermocouple
- Replies: 17
- Views: 19135
Re: Thermocouple
Thank you Kevin, it just failed. E-1 at 887 Olympic installed the elements into the lid, could they have put in the wrong ones??? How would I know that they are the wrong elements. Olympic set up the lid so that all I had to do was connect the new lid. They did almost sent the wrong relay switch but...