Search found 231 matches
- Sun Nov 01, 2015 6:30 am
- Forum: Kiln Casting
- Topic: Plaster/silica mold improvements
- Replies: 9
- Views: 28425
Re: Plaster/silica mold improvements
Les, I agree that Zircar's a good place to look, but the problem isn't so much the mold as the release at prolonged temperatures of 2100F or thereabouts. MM6 might hold up, but I'm not sure I'd trust either kilnwash or most of the BN sprays I'd like to do some experimenting with paper clay under no...
- Mon Apr 20, 2015 3:31 am
- Forum: Art, philosophy, and content
- Topic: Silence
- Replies: 26
- Views: 393483
Re: Silence
I miss Brock too and and am now worried, I see he is no longer a "member" I hope its only temporary . Facebook groups Yes, there are some answers that are just plan scary; given to questions on Facebook's sites. Folks acting knowledgeable and/or authoritative - with very little experience ...
- Wed Feb 04, 2015 4:20 am
- Forum: Kiln Casting
- Topic: Plaster mold
- Replies: 11
- Views: 41076
Re: Plaster mold
I found a place that does aluminum casting and sells the investment. I have contacted them to buy some. I'll let you know!
http://www.avalon-castings.com/investme ... g/aluminum
http://www.avalon-castings.com/investme ... g/aluminum
- Wed Feb 04, 2015 3:46 am
- Forum: Techniques and Tools
- Topic: Vitrograph Kiln set up
- Replies: 5
- Views: 13094
Re: Vitrograph Kiln set up
I also use a vermiculite board, drilled a hole in it, I sat that on an old kiln shelf with a hole. I was worried about it cracking hence the kiln shelf under it. I also use a coller with my caladra so I can use taller pots.
Hope this is of some help
Shereen
Hope this is of some help
Shereen
- Mon Feb 02, 2015 10:50 pm
- Forum: Kiln Casting
- Topic: Plaster mold, 1st time questions
- Replies: 13
- Views: 42937
Re: Plaster mold, 1st time questions
I just love this board , I googled my question and such wonderful artists chime in. Thank you !
- Wed Jan 28, 2015 6:31 am
- Forum: Techniques and Tools
- Topic: Quenching glass
- Replies: 22
- Views: 50037
Re: Quenching glass
Hello neighbor ,
I bought an old SS MILK bucket and make Frit. Ann nye posted a video how she (well her husband) does it,
https://m.youtube.com/watch?v=p3mpWIv08lc
Enjoy the rain we've been getting!
Shereen
I bought an old SS MILK bucket and make Frit. Ann nye posted a video how she (well her husband) does it,
https://m.youtube.com/watch?v=p3mpWIv08lc
Enjoy the rain we've been getting!
Shereen
- Sun Jan 11, 2015 4:12 am
- Forum: Newcomer Forum
- Topic: Has anyone perfected opaque frit balls?
- Replies: 11
- Views: 41990
Re: Has anyone perfected opaque frit balls?
I use Coca-Cola to remove it.
- Sun Jan 11, 2015 4:10 am
- Forum: Techniques and Tools
- Topic: Where to buy ceramaguard
- Replies: 4
- Views: 10754
Re: Where to buy ceramaguard
Anyplace that sells Armstong ceiling tiles. If you need to buy more than you need i
I'll buy part of the box. My parents are in SF,
http://www.armstrong.com/commceilingsna ... -cZ1z141dp
I'll buy part of the box. My parents are in SF,
http://www.armstrong.com/commceilingsna ... -cZ1z141dp
- Sun Jan 11, 2015 4:06 am
- Forum: Kiln Casting
- Topic: Mold bits in my casting
- Replies: 4
- Views: 18002
Re: Mold bits in my casting
Cynthia, when are you going to take all your words of wisdom and have it typed up into a book? I'll bet most of its out there and you just need to organize it?
Sign me up please ..
Sign me up please ..
- Thu Jan 08, 2015 8:58 am
- Forum: Techniques and Tools
- Topic: Making a mold of a bowl
- Replies: 18
- Views: 43754
Re: Making a mold of a bowl
Thank you Dana, The customer is still in Europe so as soon as they sail back I'll share this mold . I'll check bluefure contact info and call them about the size. I doubt my customer cares but it would be much cheaper to use a ready made mold. I'm still going to do the clay process as I love to lear...
- Mon Jan 05, 2015 8:18 am
- Forum: Techniques and Tools
- Topic: Making a mold of a bowl
- Replies: 18
- Views: 43754
Re: Making a mold of a bowl
Thank you all so much, what I've decided to do is carve the shape on a leather hard 14" round peice of clay. Fire it with vent holes. Pre fire a 1/4 in piece of glass and then use the mold with enamels/frit. Then slump it. Would screening enamels over the prepared mold be better than using frit...
- Sat Jan 03, 2015 5:17 am
- Forum: Techniques and Tools
- Topic: Making a mold of a bowl
- Replies: 18
- Views: 43754
Re: Making a mold of a bowl
Morginia , That's a great idea, I am going to change it a bit and they don't want clear. The colors are yellow/brown to go with green plates. Not my choice tho' however it's not as bad as the customer who wanted a full size ferret SG window a few years back for her bedroom window. Thank you very muc...
- Fri Jan 02, 2015 8:50 am
- Forum: Techniques and Tools
- Topic: Making a mold of a bowl
- Replies: 18
- Views: 43754
Making a mold of a bowl
Hello, Is it possible to make a mold of the inside of a bowl and utilize it? I was approached and asked if I could make 12 salad bowls just like this bowl which is made if some type of hard plastic. I do have a quart of silicon mold as well as ceramic mold and clay. Thank you Shereen My new year res...
- Fri Dec 19, 2014 3:26 am
- Forum: Techniques and Tools
- Topic: cloth "molds"
- Replies: 9
- Views: 19694
Re: cloth "molds"
I have some lava cloth and have used it make nice designs in glass. The ceramic lava cloth worked well for me, I wonder if it was different than the cloth you bought. I'll take a photo of the glass and post it.
Shereen
Shereen
- Thu Dec 18, 2014 1:30 am
- Forum: Techniques and Tools
- Topic: Hanovia Gold
- Replies: 11
- Views: 24811
Re: Hanovia Gold
Thank you all, Yes I did mean .02 bottles - I wrote kathy and she replied very quickly - here are her instructions (I know how much the search tool has helped me in the past) The proper thinner for Bright Gold is the OH1 Essence $9.95/1/2 oz. It is made by the gold Factory and is the only thing I wo...
- Sun Dec 14, 2014 4:26 am
- Forum: Techniques and Tools
- Topic: Hanovia Gold
- Replies: 11
- Views: 24811
Hanovia Gold
Hello, I was given a dozen 2oz bottles of Hanovia gold and most of them need thinning- 2 are completely dry. They are (or were) sealed up and looking at the prices on them they are fairly old. I don't want to experiment putting something like clove oil if its not the correct thing. Does anyone know ...
- Thu Oct 09, 2014 4:37 am
- Forum: Newcomer Forum
- Topic: MAgazines
- Replies: 5
- Views: 17714
Re: MAgazines
Mike, If youre looking for magizines to learn techniques - one of the best deals are bullseye's online video education http://www.bullseyeglass.com/education/bullseye-kiln-glass-education-online.html Lots of free videos and you have access to all the past ones. Lastly, several months ago I bought 50...
- Sun Aug 24, 2014 6:03 pm
- Forum: Techniques and Tools
- Topic: Blaster Question
- Replies: 12
- Views: 25430
Re: Blaster Question
Jim, I too have the same standing cabinet, you might find this video helpful as he does some modifications of his cabinet. The issues I fixed right off was the poor lighting and the nozzle. Both of these are easily fixes. My next task is sealing areas where AO leaks a bit. Good luck https://m.youtub...
- Fri Jul 11, 2014 5:06 am
- Forum: Techniques and Tools
- Topic: 3d printers
- Replies: 5
- Views: 11540
3d printers
With 3d printers getting cheaper and larger Im very tempted to get one. What can a glass artist use one for? Besides making designs you can then make a mold with.
Thank you
Shereen
Thank you
Shereen
- Fri Jun 13, 2014 3:01 am
- Forum: Techniques and Tools
- Topic: Real gold
- Replies: 5
- Views: 11700
Re: Real gold
yes its all sealed -he sent me four boxes of it. Thank you for the link!
Id love to use it to draw on glass and fuse it!
Shereen
Id love to use it to draw on glass and fuse it!
Shereen