Search found 1 match

by Mara
Mon Jun 02, 2003 2:40 am
Forum: Techniques and Tools
Topic: Large bubble on my 20" diameter piece
Replies: 15
Views: 25951

Marty, I took a look at the piece this afternoon and found another golfball size bubble after the second firing. This bubble was closer to the center, but occured where there were only two layers rather than three. Talked to two glass artist, one suggested 1500 was too hot, bring down to 1450 and so...