Re: ISO Metal Spinner
I used a small ss cup, ground off the rolled edge and made the edge as thin as possible then put it over a small clay pot. Pressed down hard to make sure it did not come off, kw it all and presto had a set to fill the kiln and make draped vases. You could do the same with a tall ss cocktail shaker a...
- Wed Sep 19, 2012 2:46 pm
- Forum: Techniques and Tools
- Topic: LIQUID GLASS................CMC.............Alternatives
- Replies: 31
- Views: 36063
Re: LIQUID GLASS................CMC.............Alternatives
Cynthia: Your stories sound interesting. Are they on your blog? Would love to read them. Georgia
- Wed Sep 19, 2012 2:40 pm
- Forum: Techniques and Tools
- Topic: MESH MELT DISASTER
- Replies: 21
- Views: 21304
Re: MESH MELT DISASTER
Jim: I see the re-bar but do not know what the mesh is. Is it SS? If so where do you purchase it? Thanks, Georgia
- Sun Sep 02, 2012 6:25 pm
- Forum: Techniques and Tools
- Topic: Wearing gloves when cutting glass
- Replies: 17
- Views: 29026
Re: Wearing gloves when cutting glass
It sounds like you are cutting at an angle or cutting a lot of textured glass. There is a stick...it is about 8" long x3/4x1", I cann't remember the name of it I've had it for so long. After cutting you run it along the edges and it knocks off all the razor bevels and point spurs. I use it...
- Mon Aug 27, 2012 5:01 pm
- Forum: Newcomer Forum
- Topic: MESH MELT
- Replies: 23
- Views: 32188
Re: MESH MELT
Immerman of Clear Water Glass Studio uses hardware cloth (Rabbit cage wire) for his wire melts. Isn't that galvanized? Georgia
- Thu Aug 02, 2012 4:07 pm
- Forum: Techniques and Tools
- Topic: how to remove silicone glue?
- Replies: 9
- Views: 10720
Re: how to remove silicone glue?
Many years ago when I first started stained glass, I glued a panel into the grooved out area of a wooden door, per instructions of teacher. Well, or course a piece broke and the panel had to be removed. I wrote to e-6000 and asked how. They sent me a list in order from weak to strong. I think I fina...
- Fri Aug 29, 2003 1:48 am
- Forum: Photos and Stuff
- Topic: magnet exchange pictures
- Replies: 12
- Views: 14104
- Fri Aug 15, 2003 5:58 pm
- Forum: Photos and Stuff
- Topic: magnet exchange pictures
- Replies: 12
- Views: 14104
magnet exchange pictures
I am looking for pictures of the last magnet exchange. Can not find it please help.
Georgia
Georgia