I've been using it and love it. Doing jewelry, so maybe smaller pieces than some of you but I have not experienced any sticking to opals or otherwise. I got 5 firings out of the last sheet I laid down. I will be buying more. I also like the fact that there is not a could of dust after the firing, ju...
- Sun Aug 26, 2012 12:21 am
- Forum: Jewelry Making
- Topic: fusible yoga decals? (ohm maybe or namaste)
- Replies: 5
- Views: 10142
Re: fusible yoga decals? (ohm maybe or namaste)
Have you tried "glimmerglassgifts" ?
- Fri Aug 17, 2012 12:34 am
- Forum: Techniques and Tools
- Topic: Molds are there better Molds?
- Replies: 10
- Views: 13045
Re: Molds are there better Molds?
Thanks Dana, good to know it's not just me. This is certainly not what I was lead to believe would happen. It's kind of a novelty and I wanted to give it a try but not impressed.
Carol
Carol
- Thu Aug 16, 2012 8:37 pm
- Forum: Techniques and Tools
- Topic: Molds are there better Molds?
- Replies: 10
- Views: 13045
Re: Molds are there better Molds?
Just used a Color de Verre mold for the 1st time. Followed the directions to the letter and still has a slightly stuck piece. I was able to get it out and maybe it was my fault and I didn't have an even coat of BN. What I don't like is the rough texture and spikes on some pieces even though I was ve...