Search found 1 match

by Nonnie
Sat Dec 28, 2013 2:58 pm
Forum: Techniques and Tools
Topic: Devit Problem with BE
Replies: 21
Views: 61103

Re: Devit Problem with BE

Sprinkle a thin coat of BE clear powder over the project before firing and you will prevent the devit. I do it on almost every project, but ALWAYS with BE reds, blues, and purples.