Search found 13 matches

by MarkNotMarc
Wed Jun 08, 2016 1:11 am
Forum: Business Topics
Topic: New Bullseye Status
Replies: 7
Views: 36585

Re: New Bullseye Status

This is good news for glass, lets hope Urobouros is able to take advantage of the same deal.

Just got notice from Bullseye, prices are going up 12.5% or something like that, starting August I believe.

Guess we are all going to pay for it. Still better than no glass at all.

Long live studio glass!
by MarkNotMarc
Thu Jul 16, 2015 4:59 pm
Forum: Kiln Casting
Topic: Mixing large amounts of dry plaster and silica
Replies: 14
Views: 58896

Re: Mixing large amounts of dry plaster and silica

why would you mix that dry? you will never get an even mix so your castings would be un predictable. you slake the proper proportions into water when making molds. the mix happens in the water. r. I disagree, dry mixing will give a better plaster/silica distribution than just scooping both into wat...
by MarkNotMarc
Tue Jul 14, 2015 9:52 pm
Forum: Kiln Casting
Topic: Mixing large amounts of dry plaster and silica
Replies: 14
Views: 58896

Re: Mixing large amounts of dry plaster and silica

depends on what you mean by large amounts? You could use a 5 gallon plastic bucket with a lid and roll it around on the floor. For larger quantities get a cement mixer and fabricate a plywood lid with toggle clamps to hold it on. I have heard it works best if you remove the interior blades from the ...
by MarkNotMarc
Sun Jun 21, 2015 9:10 pm
Forum: Techniques and Tools
Topic: Best deals on Paragon kilns?
Replies: 7
Views: 11357

Re: Best deals on Paragon kilns?

As mentioned Bullseye has a good sale going on, but you have to walk into one of their 4 locations to get the deal. No on line orders. (or so they say) Most of the big online ceramic supply stores will sell a variety of kiln brands including Paragon. Sign up for their mailing list to hear about the ...
by MarkNotMarc
Mon May 11, 2015 1:07 pm
Forum: Techniques and Tools
Topic: Ode to kiln controllers...
Replies: 12
Views: 19118

Re: Ode to kiln controllers...

Cynthia,

Maybe you just need a side hobby like throwing ceramic mugs (on the potters wheel, not at the wall) lol

Mark
by MarkNotMarc
Wed May 06, 2015 2:27 am
Forum: Kiln Casting
Topic: Bruno Romanelli Glass casting
Replies: 4
Views: 9286

Bruno Romanelli Glass casting

This video is a couple years old but thought folks might enjoy.

http://vimeo.com/51354144

Mark
by MarkNotMarc
Wed Sep 03, 2014 3:55 am
Forum: Newcomer Forum
Topic: What do I put Bullseye transparent frit on?
Replies: 9
Views: 12902

Re: What do I put Bullseye transparent frit on?

The COE number of all glass fused into one piece should be the same COE number. Don't mix 90 and 96 in the same piece. Many people say not to mix the same COE from different manufacturers. Your results may vary. Bullseye frit is designed to work with Bullseye fusing sheet glass. Just don't use it wi...
by MarkNotMarc
Tue Mar 18, 2014 1:45 pm
Forum: Photos and Stuff
Topic: New Colour Bar project
Replies: 47
Views: 53916

Re: New Colour Bar project

Les, Thank you for reconsidering leaving the forum. Your work is inspiring and I along with so many others on this board really, really, really appreciate your contributions, knowledge and experience. Thanks for sharing your work and your process shots they are so educational (and beautiful). I did ...
by MarkNotMarc
Mon Feb 10, 2014 11:10 pm
Forum: Techniques and Tools
Topic: Wax Vac, no its not what you think!
Replies: 12
Views: 15602

Re: Wax Vac, no its not what you think!

Oh, I know...the new blog is actually not live yet, so you couldn't possibly have seen it. I saw your post right after I'd test-published that review to see if things were working. Got a kick out of the coincidence, too much not to share. Great minds think alike, I guess... ;-) What, what, what!!! ...
by MarkNotMarc
Fri Dec 13, 2013 10:25 pm
Forum: Photos and Stuff
Topic: Damascus, Arizona
Replies: 17
Views: 22977

Re: Damascus, Arizona

Don Burt wrote:Thanks Peter. Yes I made the frame.
Not sure what the appropriate response is to your question Bert. I'm weak on Monty Python.
You could say "Are all your pets named Eric?" tell me about your pet "half a bee" named Eric.
by MarkNotMarc
Mon Nov 11, 2013 11:15 pm
Forum: Techniques and Tools
Topic: Removing glass plug from diamond drill bit
Replies: 25
Views: 32689

Re: Removing glass plug from diamond drill bit

You have to drill those out with smaller 2mm drills they come right out, but then you need to clear the 2mm drill bit so i guess that means 1mm bits. - haha

Cynthia is right, let me know if you figure it out.
by MarkNotMarc
Fri Oct 25, 2013 11:15 am
Forum: Techniques and Tools
Topic: Share your water drip techniques and methods
Replies: 9
Views: 14548

Re: Share your water drip techniques and methods

Thanks for all the suggestions!
by MarkNotMarc
Wed Oct 23, 2013 1:29 pm
Forum: Techniques and Tools
Topic: Share your water drip techniques and methods
Replies: 9
Views: 14548

Share your water drip techniques and methods

I am starting to grind off the flashing from a kiln cast sculpture using a Foredom hand grinder with diamond burrs. I want to keep the burr wet without working underwater and would like to hear what others have come up with for a water feed drip system. I thought of using an IV bag, or even a 2 gall...