Search found 24 matches
- Mon Oct 09, 2017 1:17 pm
- Forum: Techniques and Tools
- Topic: precious metal clay
- Replies: 6
- Views: 10374
precious metal clay
I am thinking of adding some embellishments to a piece with pieces of precious metal clay. will the clay fuse to the glass? or will the glass crack because of incompatibility issues?
- Thu May 19, 2016 2:35 pm
- Forum: Newcomer Forum
- Topic: Cooling small glass pieces - AFAP?
- Replies: 7
- Views: 14573
Re: Cooling small glass pieces - AFAP?
I Have a firebox 8 with out a fancy controller, for small pieces I just ramp it up hold and turn it off . It naturally cools down so slow that it has never been an issue.
- Thu May 19, 2016 2:22 pm
- Forum: Techniques and Tools
- Topic: WHAT HAPPENNED HERE?
- Replies: 4
- Views: 7727
Re: WHAT HAPPENNED HERE?
are you crash cooling your kiln?9 letting it get to the anneal hold with the lid open) That can cause the bricks to crack and eventually start to fall apart.
- Tue May 10, 2016 8:03 pm
- Forum: Techniques and Tools
- Topic: split glass
- Replies: 8
- Views: 9820
Re: split glass
I refired the piece today and it looks good. thank you Brad you were right.
- Mon May 09, 2016 12:42 pm
- Forum: Techniques and Tools
- Topic: split glass
- Replies: 8
- Views: 9820
Re: split glass
I really don't think it was the anneal . my schedules are very concretive and have worked very well until now . I am prone to believe that it was not enough heat because for the first part of the slump everything was fine but as it started to drop down into the lower part of the mold it started to s...
- Sun May 08, 2016 3:23 pm
- Forum: Techniques and Tools
- Topic: split glass
- Replies: 8
- Views: 9820
Re: split glass
ok. since it did not break into separate pieces I was able to flatten and heal the piece. so I guess a longer hold at the 1000 point should take care of the problem when I re slump it?
- Sat May 07, 2016 4:13 pm
- Forum: Techniques and Tools
- Topic: split glass
- Replies: 8
- Views: 9820
Re: split glass
thanks that makes sense.
- Sat May 07, 2016 12:50 pm
- Forum: Techniques and Tools
- Topic: split glass
- Replies: 8
- Views: 9820
split glass
My screen melt split about 10 minutes into the slump. I am assuming that there was not enough heat in the glass , and therefore the split. I was wondering though weather there could be some other factors that could have caused it? my schedule was as follows 200/1000 30 50/ 1150/ 30 this was a 3/8 th...
- Fri Oct 16, 2015 9:39 am
- Forum: Techniques and Tools
- Topic: melting frit to make a single piece of glass
- Replies: 8
- Views: 13309
melting frit to make a single piece of glass
If I take glass that is from the same company, in this case Kokomo and frit scrap pieces( not necessarily from the same sheet ) but the same color into a fine frit, and than take them up to a full fuse in a mold and form 1 piece of glass will they be compatible since I have now made a single piece o...
- Wed Jul 22, 2015 10:59 am
- Forum: Techniques and Tools
- Topic: float glass
- Replies: 8
- Views: 13349
Re: float glass
Thanks
- Wed Jul 22, 2015 8:18 am
- Forum: Techniques and Tools
- Topic: float glass
- Replies: 8
- Views: 13349
float glass
If I stack 3 or 4 pieces of float glass together and tack fuse them and then do a shallow slump will I get float bloom between the layers of glass? I am thinking of sandblasting the various layers before I fuse them to see if I can get some depth. will the sandblasted image's remain in the glass at ...
- Tue May 05, 2015 2:17 pm
- Forum: Techniques and Tools
- Topic: screen melt sticking to mold
- Replies: 8
- Views: 8429
Re: screen melt sticking to mold
THANK YOU
- Tue May 05, 2015 11:09 am
- Forum: Techniques and Tools
- Topic: screen melt sticking to mold
- Replies: 8
- Views: 8429
Re: screen melt sticking to mold
Keven after reading your reply, I re examined both the mold and the piece, and I noticed that the areas of the glass that are affected are indeed the thicker parts of the piece. and there are small pin point holes in the kiln wash in the mold. can this be avoided in the future with Boron nitrate and...
- Tue May 05, 2015 10:35 am
- Forum: Techniques and Tools
- Topic: screen melt sticking to mold
- Replies: 8
- Views: 8429
Re: screen melt sticking to mold
actually I thought 200dph was pretty slow. what temp would you suggest
- Tue May 05, 2015 9:17 am
- Forum: Techniques and Tools
- Topic: screen melt sticking to mold
- Replies: 8
- Views: 8429
Re: screen melt sticking to mold
for this one I went to 1240 and held for about 20 min I used primo primer on both molds . on the stainless I heated it up first and than sprayed several coats of the primer until I got a nice smooth coat I used 1240 because when I flattened out the first slump it did not flatten until 1230 also this...
- Tue May 05, 2015 8:07 am
- Forum: Techniques and Tools
- Topic: screen melt sticking to mold
- Replies: 8
- Views: 8429
screen melt sticking to mold
I just did a screen melt, onto a piece of clear turned out great , turned out to be about 3/8 thick I cold worked it and took it up to a full fuse, ended up with a really pretty piece . problem is when I slumped it in a ceramic mold the edges caught in a couple of places and it did not slump evenly....
- Mon Feb 23, 2015 11:41 pm
- Forum: Techniques and Tools
- Topic: damaged kiln shelf
- Replies: 7
- Views: 11733
Re: damaged kiln shelf
there is a product called patch a tach used for repairing bisk ware. I have used it to repair molds and fill in scratches in my kiln shelf it can be found through most ceramic supply houses cheep and easy fix
- Sun May 18, 2014 4:44 pm
- Forum: Techniques and Tools
- Topic: vasoline glass
- Replies: 5
- Views: 6853
Re: vasoline glass
THANKS.
- Sun May 18, 2014 2:12 pm
- Forum: Techniques and Tools
- Topic: vasoline glass
- Replies: 5
- Views: 6853
vasoline glass
I have some glass that by a slight chance might be Vaseline glass I can't seem to locate a black light to check it out . I would like to use it in some pod molds and was wondering if there were any hazards I should be aware of either to me or the kiln.
- Tue May 13, 2014 10:31 pm
- Forum: Techniques and Tools
- Topic: Getting indentations
- Replies: 10
- Views: 10505
Re: Getting indentations
this mold makes for a subtle effect, it looks best using cathedral or clear glass that you can see the design from the top other wise it is not very impressive as a design on the bottom ofa piece