Search found 6 matches
- Tue Apr 02, 2013 11:12 am
- Forum: Techniques and Tools
- Topic: Does this Firing schedule sound ok?
- Replies: 12
- Views: 15043
Re: Does this Firing schedule sound ok?
I've managed to fire the panels successfully thanks to all the advice! Cynthia I use a combination of leaf and powders.
- Tue Mar 26, 2013 3:20 am
- Forum: Techniques and Tools
- Topic: Does this Firing schedule sound ok?
- Replies: 12
- Views: 15043
Re: Does this Firing schedule sound ok?
Hi Bert I've decided to increase my schedule in the 615 region and also up to fuse temp like you've suggested. My cooling/ annealing sections are longer so, given the inaccuracy of my kiln I think I'll keep it as it is to be on the safe side and then do a test fire. A thermocouple that is encased in...
- Mon Mar 25, 2013 9:45 am
- Forum: Techniques and Tools
- Topic: Does this Firing schedule sound ok?
- Replies: 12
- Views: 15043
Re: Does this Firing schedule sound ok?
Thanks Bert, as I said my kiln fires 55 degrees C lower than the controller shows. I arrived at this conclusion by placing 8 cones inside and watching throw the vent hole to see when the 810 c bent. I live in the country side so the electricity supply is erratic and also I know my controller isn't c...
- Mon Mar 25, 2013 4:18 am
- Forum: Techniques and Tools
- Topic: Does this Firing schedule sound ok?
- Replies: 12
- Views: 15043
Re: Does this Firing schedule sound ok?
My mistake, I mean't 50mm (5cm) great Idea to test fire clear.....Thanks Stephen 
- Sun Mar 24, 2013 1:00 pm
- Forum: Techniques and Tools
- Topic: Does this Firing schedule sound ok?
- Replies: 12
- Views: 15043
Re: Does this Firing schedule sound ok?
Ah, well there's about 110mm distance gap from the edge on the long sides and about 5mm top and bottom edges. I also tend to reinforcing all side ( about 30mm from the piece with used ceramic fiber paper rolled up, as I've found that my kiln doesn't heat evenly. ( It's a fiber board and brick laser ...
- Sun Mar 24, 2013 10:38 am
- Forum: Techniques and Tools
- Topic: Does this Firing schedule sound ok?
- Replies: 12
- Views: 15043
Does this Firing schedule sound ok?
I'm about to fire 2 large panel measuring 1metre x 50cm each. One at a time. I'm fusing metals in leaf and foil forms between two sheets of 3mm float. I've placed spacers at each corner to allow the metals to fuse in properly and prevent burnout. My question is do you think this firing schedule soun...