Search found 27 matches
- Wed Apr 25, 2018 8:28 am
- Forum: Techniques and Tools
- Topic: Slumping issues
- Replies: 17
- Views: 33948
Re: Slumping issues
Why hold (and why there) at all for a simple slump? What's going to happen? My previous "go to" schedule was not far from yours, although I ramped at 300 per. As mentioned, I had issues with certain molds slumping unevenly. Maybe the design of the mold. Who knows, who cares. Frustrating t...
- Tue Apr 24, 2018 3:31 pm
- Forum: Techniques and Tools
- Topic: Slumping issues
- Replies: 17
- Views: 33948
Re: Slumping issues
I would hardly call a 20 min hold at 1100 elaborate.Marty wrote:No need for elaborate holds at 1100 etc.
- Sat Apr 21, 2018 11:04 am
- Forum: Techniques and Tools
- Topic: Slumping issues
- Replies: 17
- Views: 33948
Re: Slumping issues
My slumping schedule is more conservative. I've had issues with uneven slumping and slowed way down. I'll ramp @ 300 per to 1100 and hold for 20 min to ensure an even soak then ramp to 1250 @ 50 per. No issues to date. Also, make sure your kiln and shelf are as level as can be.
- Wed Jan 24, 2018 10:17 am
- Forum: Techniques and Tools
- Topic: Trying to find relay for kiln
- Replies: 2
- Views: 7650
Re: Trying to find relay for kiln
If you've never done this before, unplug the kiln before removing the relay to be sure all power is off! Mark the wires so they are re-attached properly. Take a picture, make a drawing... whatever. Just replaced a relay on my Olympic kiln. Called them and had it in a few days. Not outrageously expen...
- Tue Jan 31, 2017 2:24 pm
- Forum: Photos and Stuff
- Topic: First plate finished.
- Replies: 7
- Views: 29472
Re: First plate finished.
Nice job! Kudos.
- Tue Jan 31, 2017 2:18 pm
- Forum: Techniques and Tools
- Topic: 11" disc - 12" mold
- Replies: 4
- Views: 9680
Re: 11" disc - 12" mold
You could use a circular bubble level to ensure the glass is parallel to your shelf. If the top of your mold is flat and even all the way around, you could put a straight edge across the mold and measure the distance to the glass. Do this at 3 or 4 points around your piece. If your slumping temp is ...
- Thu Dec 15, 2016 12:38 pm
- Forum: Techniques and Tools
- Topic: Slumping 2 mil glass
- Replies: 12
- Views: 26337
Re: Slumping 2 mil glass
I don't often add my 2 cents for firing questions as there are more knowledgeable people here than me but, from an engineering perspective, I have a couple of thoughts. First, i think draping it would give you the most consistent shape, take less steps and give you a wider range of materials to use....
- Fri Nov 18, 2016 5:51 am
- Forum: Techniques and Tools
- Topic: Kiln paper after it's fired
- Replies: 4
- Views: 11453
Re: Kiln paper after it's fired
I keep a 5 gallon bucket of water near my kiln half filled with water. I periodically add to it to keep a level. When i'm done firing, I tilt the shelf over the bucket and usually the whole piece slides off the shelf. Sometimes I have to help it with a plastic spatula. You don't want to scratch your...
- Wed Apr 09, 2014 7:47 pm
- Forum: Techniques and Tools
- Topic: Ideas for Easter Egg Fun
- Replies: 7
- Views: 14098
Re: Ideas for Easter Egg Fun
Sorry to be dense here, but: What are the 'pre-cut' eggs of which you speak? What do you mean when you say "split them in half?" Thanks! We "pre-cut" the eggs before the kids arrived. 3 mm ovals in various colors. And all the "adornments" were ready at their disposal. ...
- Tue Apr 08, 2014 3:50 pm
- Forum: Techniques and Tools
- Topic: Ideas for Easter Egg Fun
- Replies: 7
- Views: 14098
Ideas for Easter Egg Fun
A few years ago, my wife and I invited some friends over with kids who seemed bored with the same ole egg dye this time of year. We set up egg decorating stations with pre-cut eggs, split some in half and supplied various cups with frit, stringers, noodles and an assortment of glass bits for decorat...
- Sun Feb 09, 2014 8:59 pm
- Forum: Newcomer Forum
- Topic: Ben & Vanessa's Newcomer Questions and Endless Posts
- Replies: 41
- Views: 142130
Re: Ben & Vanessa's Newcomer Questions and Endless Posts
I will NEVER give up my soldering iron I tell you, NEVER!

- Tue Feb 04, 2014 9:19 am
- Forum: Newcomer Forum
- Topic: Glassline Paper - need advice about hold time
- Replies: 12
- Views: 35910
Re: Glassline Paper - need advice about hold time
Lori, I would anneal at your normal temp. Don't change when you've had success. I use System 96 so everything get annealed at 950. If you use COE 90, anneal at what is recommended for that glass. The paper used in the glassline paper is just thinfire. The "textured" paper is wrinkled thinf...
- Mon Feb 03, 2014 1:01 pm
- Forum: Newcomer Forum
- Topic: Glassline Paper - need advice about hold time
- Replies: 12
- Views: 35910
Re: Glassline Paper - need advice about hold time
The 4 hours@ 1000 seems long but I believe it is for the paper to burn out. Use chads so you don't trap air and gasses during this step. It's been my experience that the manufacturer's schedule is fine for small pieces (refrigerator magnet size), but for large pieces like yours (6.5"), definite...
- Sat Aug 03, 2013 10:02 pm
- Forum: Photos and Stuff
- Topic: Stripcut and other techniques
- Replies: 8
- Views: 15835
Re: Stripcut and other techniques
Wow, i am inspired! I love it!
- Sat Aug 03, 2013 9:59 pm
- Forum: Photos and Stuff
- Topic: Finished window project
- Replies: 7
- Views: 16561
Re: Finished window project
Very impressed! Beautiful work.
- Thu Jul 25, 2013 7:18 pm
- Forum: Photos and Stuff
- Topic: Some Recent Work To Say Thanks
- Replies: 11
- Views: 23637
Re: Some Recent Work To Say Thanks
Thanks to you all for the kind comments.
De Nada (No problem) tbach.
De Nada (No problem) tbach.
- Wed Jul 24, 2013 10:45 am
- Forum: Photos and Stuff
- Topic: Some Recent Work To Say Thanks
- Replies: 11
- Views: 23637
Re: Some Recent Work To Say Thanks
Thank you valerie.
Yes. Interesting, isn't it? She's a cute kid though. Hopefully she won't have a bumpy road over it.Valerie Adams wrote:Now, if only we could do something about that poor girl's name...
- Tue Jul 23, 2013 7:19 pm
- Forum: Photos and Stuff
- Topic: Some Recent Work To Say Thanks
- Replies: 11
- Views: 23637
Re: Some Recent Work To Say Thanks
Thank you Joyce. Thank you tbach. The materials I used were Dichro slide and Decal sheet material. Each piece was cut using Exacto blades and scissors. Change blades often! It is not fusible Photo paper. I purchased from GlassArtPatterns.com. They have good tutorials on how to use this. It comes in ...
- Tue Jul 23, 2013 8:28 am
- Forum: Photos and Stuff
- Topic: Some Recent Work To Say Thanks
- Replies: 11
- Views: 23637
Some Recent Work To Say Thanks
Every year, my wife and I fish in a tag and release fishing tournament that benefits the The Large Pelagics Research Center (LPRC) to help continue research of Bluefin Tuna's spawning habits, migration habits, growth patterns and general species well-being. The event organizer of many years and Blue...
- Thu May 09, 2013 10:01 pm
- Forum: Techniques and Tools
- Topic: Mold Storage Ideas
- Replies: 5
- Views: 11161
Re: Mold Storage Ideas
I use bubble wrap (with the small bubbles) folded in half and taped on the edges to create a pouch that is custom sized for each mold. Stack them without worry of scratches. A large roll at an office supply store is fairly inexpensive and I always have some on hand to wrap glass for gift giving.