Search found 4 matches

by rfreedfl
Mon Mar 04, 2013 10:07 pm
Forum: Techniques and Tools
Topic: Tack fusing a tall stack
Replies: 2
Views: 7623

Tack fusing a tall stack

I want to make candlesticks. I have fired multiple 2 layer pieces and want to stack them (staggered) and tack fuse them. Is this possible? If so, should they all be fired at once? Would I be better off gluing them or is there an alternate method to stack and attach them that someone could suggest? T...
by rfreedfl
Sun Feb 10, 2013 11:34 am
Forum: Techniques and Tools
Topic: designing & firing a 5 layer project
Replies: 23
Views: 52860

Re: designing & firing a 5 layer project

Thanks to everyone for your help. I fired the piece using Cynthia's method and was successful. My reasoning for this was that my kiln has both side and top elements. My dam was made of fiber paper which I believed would be an insulator. I thought that having the one single layer on the bottom, less ...
by rfreedfl
Fri Feb 01, 2013 5:04 pm
Forum: Techniques and Tools
Topic: designing & firing a 5 layer project
Replies: 23
Views: 52860

Re: designing & firing a 5 layer project

Thanks Rose. Yes I plan to dam the piece. It's an odd shape so I plan to dam it using cut out fiber paper. Should this be 2-3 mm shorter than the finished piece, or the height of the finished piece? Do I understand correctly that you are recommending pre-firing 1 - 2 layer and 1 - 3 layer stack( wit...
by rfreedfl
Thu Jan 31, 2013 4:16 pm
Forum: Techniques and Tools
Topic: designing & firing a 5 layer project
Replies: 23
Views: 52860

designing & firing a 5 layer project

I am attemping to make a 5 layer project. I will have 1 patterned glass layers with 2 layers of clear top and bottom. I am planning to pre-fire 2 double layers (2 3mm sheets) first. #1 Should I pre-fire the patterned layer to one sheet of clear, or fire the 2 sets of 2 clear layers and place the pat...