Search found 3 matches

by hifire
Sun Jun 10, 2012 9:47 pm
Forum: Newcomer Forum
Topic: Slumping 24" x 24" tack fused COE 96 glass
Replies: 6
Views: 17773

Re: Slumping 24" x 24" tack fused COE 96 glass

I must say, I was incredibly amazed that they would ship glass like that. And then the woman was defensive when I called her about it. I am very happy to have another source to purchase from.
nb, hifire
by hifire
Wed Jun 06, 2012 10:15 am
Forum: Newcomer Forum
Topic: Slumping 24" x 24" tack fused COE 96 glass
Replies: 6
Views: 17773

Re: Slumping 24" x 24" tack fused COE 96 glass

Okay!!! Thank you so much all for your help. I am going to go ahead and order the big sheets!! Luckily my kiln is very large so I will be able to keep the glass away from the elements. I understand that you can't really stack glass between shelves, as it changes the thermal shock. So I plan on firin...
by hifire
Tue Jun 05, 2012 11:06 am
Forum: Newcomer Forum
Topic: Slumping 24" x 24" tack fused COE 96 glass
Replies: 6
Views: 17773

Slumping 24" x 24" tack fused COE 96 glass

I am new to glass slumping. I am a ceramic artist who has a commission including slumped 24" x 24" sheet glass over undulating textured clay originals (my tiles). I am about to purchase 1000 bucks worth of Spectrum COE 96 colored and clear glass, tack fuse them together and then slump them...