Search found 2 matches

by Lloyd
Mon Jul 23, 2012 9:14 pm
Forum: Kiln Casting
Topic: getting rid of bubbles
Replies: 2
Views: 6690

Re: getting rid of bubbles

Cynthia, Thanks, these are the suggestions I was hoping for, and the explanations help me experiment in viable directions. You assume correct about mold orientation. I'm casting crystal, rhubarb, and bronze and don't see much difference in bubbles between them. I air dry my mold for several days, th...
by Lloyd
Sun Jul 22, 2012 9:18 pm
Forum: Kiln Casting
Topic: getting rid of bubbles
Replies: 2
Views: 6690

getting rid of bubbles

Hi, I'm new to this site and glass casting and am wondering about soak times for getting rid of bubbles. I'm casting Reichenbach glass, pot drip into lost wax investment mold, small head about 1200g glass, billets broken into a couple pieces to fit in pot, 1525 peak temp, with 6 hr hold. Bottom of c...