Search found 1 match

by SuzannePisano
Fri Oct 05, 2012 3:59 pm
Forum: Techniques and Tools
Topic: BE kiln wash sticking to glass
Replies: 16
Views: 36473

Re: BE kiln wash sticking to glass

I always use thin fire shelf paper in addition to the kiln wash. It leaves a nice smooth surface on the back of the glass, prevents the sticking, and allows the glass to slide and slump more consistently. You can also try sprinkling alumina hydrate powder although you may miss the sides on a steep m...