Primer Pulling Away from Shelf
I am using a Hotbox 8 and Hifire kiln wash. I apply several coats of the wash, fire at 450* for first firing. Once completed, and shelf sits a day or two, then I fire small piece of 90 coe dichro capped with clear. Firing goes well. HERE IS THE KICKER. Next firing, same glass, same firing temp 1450*...
- Sat Jan 24, 2004 8:26 pm
- Forum: Techniques and Tools
- Topic: Use of PMC3 and effects on kiln
- Replies: 7
- Views: 8482
Use of PMC3 and effects on kiln
I am interested in using some PMC3 (Precious Metal Clay) to encase some cabs, but have read various places that it may have a effect on your kiln, leaving deposits, effecting heating coils, etc. Would be interested if anyone can comment on the effects, would it be wise to use shelf paper or fire dir...
- Tue Aug 19, 2003 6:22 pm
- Forum: Techniques and Tools
- Topic: Looking for Special Slumping mold and need help
- Replies: 6
- Views: 6581
Looking for Special Slumping mold and need help
I am looking for an elongated (maybe even considered oval) mold for slumping. The one I am looking for is about 16 inches long and maybe 5 inches or so wide at the largest part. I is kind of oval in shape but not a true oval. I have heard it referred to as a "bread" server shape. If you we...