Search found 5 matches

by Sue Haan
Thu Sep 22, 2022 7:44 pm
Forum: Techniques and Tools
Topic: fusing large sheets
Replies: 1
Views: 10217

fusing large sheets

I am fusing two large sheets of Bullseye White (013-30) together. They are 13" x 29". Do I need to adjust the fusing schedule due to the size?
by Sue Haan
Mon Sep 18, 2017 11:05 pm
Forum: Techniques and Tools
Topic: Using Bending Glaze
Replies: 0
Views: 108568

Using Bending Glaze

I have two tacked pieces that have devit on them. Both have dichro on them. Has anyone used Bending Glaze on dichro? Wondering if I should spray the whole piece and refire at a slumping temp. If not compatible with dichro, would brushing the bending solution on the devitted areas help, or create mor...
by Sue Haan
Sat Mar 16, 2013 3:09 pm
Forum: Techniques and Tools
Topic: Vitrigraph Kilns
Replies: 8
Views: 17891

Vitrigraph Kilns

I am interested in buying a Vitrigraph Kiln. What's the best brand?
by Sue Haan
Sun Dec 23, 2012 4:33 pm
Forum: Techniques and Tools
Topic: Screen Melts
Replies: 35
Views: 72570

Re: Screen Melts

Thanks for the warning. I have tried one screen melt, and it did make a mess in the kiln, but I didn't think about shards of glass getting into the elements. I did find a website for a company called TWP. They sell welded stainless mesh by the square foot. I ordered some and will try to make my own ...
by Sue Haan
Sun Dec 23, 2012 12:57 pm
Forum: Techniques and Tools
Topic: Screen Melts
Replies: 35
Views: 72570

Screen Melts

Can dichro or irid glass be used for a screen melt? Also, where can I buy welded stainless mesh so I can make my own screens?