Thanks JestersBaubles! I think I was either misinformed, or I misunderstood because I believe I was told that part of the benefit to using BN rather than kiln wash, was so it would have a nice glossy finish. I guess I'm scrubbing for nothing. I didn't mind the finish so much when I did flowers, but ...
- Mon Mar 11, 2013 3:10 pm
- Forum: Kiln Casting
- Topic: MR-97 mold release
- Replies: 6
- Views: 9297
MR-97 mold release
I'm using MR-97 Boron Nitride spray for my frit molds. The glass that was in contact with the mold has a satiny sheen rather than a glossy finish. The side not in contact with the mold is glossy. Am I just not getting all the mold release off? Or am I doing something wrong? How can I scrub it off? T...
- Mon Mar 11, 2013 2:37 pm
- Forum: Techniques and Tools
- Topic: Inclusions
- Replies: 9
- Views: 9473
Re: Inclusions
Thanks so much for all the great advice! I'm going to give it a go!
p.s. I didn't know that about the marbles either. Very cool.
p.s. I didn't know that about the marbles either. Very cool.
- Sun Mar 10, 2013 11:39 pm
- Forum: Techniques and Tools
- Topic: Inclusions
- Replies: 9
- Views: 9473
Inclusions
I'm interested in fusing inclusions into my glass, but it's unclear to me whether it can be done in COE 96 or COE 90 glass. Everything I read about regarding inclusions, suggests using float glass. Does that mean float glass is all I can use with inclusions? I want to add aluminum tooling foil and c...