Search found 91 matches
- Fri Jun 21, 2013 8:28 pm
- Forum: Techniques and Tools
- Topic: Organizing and inventory
- Replies: 10
- Views: 13681
Re: Organizing and inventory
Shereen, San Diego has a very active glass community. are you in touch with the Art Glass Guild in the Spanish Village Art Center? www.artglassguild.com.
- Mon May 20, 2013 10:07 pm
- Forum: Techniques and Tools
- Topic: Slumping small bowls
- Replies: 8
- Views: 10617
Re: Slumping small bowls
I have a shallow 6" heart bowl that I slump successfully with this schedule:
300/1100/20
150/1250/20
400/960/60
300/100/0
300/1100/20
150/1250/20
400/960/60
300/100/0
- Sun May 12, 2013 4:54 pm
- Forum: Techniques and Tools
- Topic: Repairing seam lines? Advice?
- Replies: 7
- Views: 8351
Re: Repairing seam lines? Advice?
I agree, the seam lines really don't seem to be much of an issue with your interesting piece of art. if they really bother you I would add something subtle to the entire background, like others have said chunks of clear or coordinating blue/green.
- Wed May 08, 2013 1:31 pm
- Forum: Techniques and Tools
- Topic: Help reusing fully fused piece
- Replies: 3
- Views: 4799
Re: Help reusing fully fused piece
I have not done this yet but I think it's fine to incorporate it into a new piece and full fuse again.
- Sun May 05, 2013 9:53 pm
- Forum: Photos and Stuff
- Topic: New Frit Painting
- Replies: 6
- Views: 9622
Re: New Frit Painting
wow David, this is simply stunning!
- Tue Apr 30, 2013 12:07 am
- Forum: Business Topics
- Topic: charging for your work
- Replies: 7
- Views: 10164
charging for your work
So I've been selling jewelry for about 8 years and am profitable every year, at least enough to keep funding my art habit! so now I am really into fusing glass and would like to add some small plates and such to my inventory. the question is how do you price this stuff? the raw materials are so expe...
- Fri Apr 26, 2013 10:52 am
- Forum: Newcomer Forum
- Topic: base glass question
- Replies: 3
- Views: 4760
Re: base glass question
I'm a newbie too but my answer is "it depends". I've done this and had instances where there is no noticeable line and also where there is a noticeable line.
- Thu Apr 25, 2013 3:35 pm
- Forum: Art, philosophy, and content
- Topic: Art and Healing at Boston's Spaulding Hospital
- Replies: 3
- Views: 8485
Re: Art and Healing at Boston's Spaulding Hospital
it's beautiful! very calming yet interesting to look at.
- Tue Apr 23, 2013 11:51 pm
- Forum: Techniques and Tools
- Topic: Oval dish suggestions
- Replies: 3
- Views: 4353
Re: Oval dish suggestions
you cut the glass pre-fuse to fit the top of the mold. so you would cut out an oval to begin with.
- Tue Apr 23, 2013 3:10 pm
- Forum: Photos and Stuff
- Topic: One Spark Glass Quilt
- Replies: 9
- Views: 11612
Re: One Spark Glass Quilt
what a fun idea. my favorite of your tiles is the one with the bears. I'm glad it was a success.
- Mon Apr 22, 2013 10:47 am
- Forum: Newcomer Forum
- Topic: magazines
- Replies: 7
- Views: 9084
magazines
are there any glass magazines that you would recommend? I'd want info such as:
new products
new techniques
tutorials
industry happenings
new products
new techniques
tutorials
industry happenings
- Sun Apr 21, 2013 11:12 pm
- Forum: Newcomer Forum
- Topic: slumping molds
- Replies: 6
- Views: 7498
Re: slumping molds
thats great info, thank you for posting
- Thu Apr 18, 2013 11:33 pm
- Forum: Photos and Stuff
- Topic: New Colour Bar Mountain Pieces
- Replies: 6
- Views: 7058
Re: New Colour Bar Mountain Pieces
they sure do - beautiful!
- Wed Apr 17, 2013 11:56 am
- Forum: Techniques and Tools
- Topic: MELT FUSED INTO CRACKLED PIECE
- Replies: 10
- Views: 10926
Re: MELT FUSED INTO CRACKLED PIECE
I have no input but wanted to say I like your artistic idea here.
- Mon Apr 15, 2013 8:11 pm
- Forum: Newcomer Forum
- Topic: Glass moved during slump
- Replies: 20
- Views: 20733
Re: Glass moved during slump
I have no idea but how frustrating!!!
- Sun Apr 14, 2013 11:23 pm
- Forum: Newcomer Forum
- Topic: Use of kiln space
- Replies: 12
- Views: 11104
Re: Use of kiln space
fire some frit grains to make little balls.
- Sun Apr 14, 2013 4:27 pm
- Forum: Newcomer Forum
- Topic: Fusing schedule question
- Replies: 11
- Views: 12926
Re: Fusing schedule question
I would say you should also ramp up slower than normal because all those layers will heat up at different rates. I am a newbie but I had a piece which was all 2 layers but I had 3 circles stacked on top. I got a crack right by the circles and my teacher told me it's because the circles were so thick...
- Sun Apr 14, 2013 4:25 pm
- Forum: Newcomer Forum
- Topic: How to make sharp lines
- Replies: 9
- Views: 9832
Re: How to make sharp lines
what if you put a clear layer on the bottom (in order to get the two required layers) and then use thinner glass for the black? then it would not spread out as much.
- Sun Apr 14, 2013 12:46 pm
- Forum: Newcomer Forum
- Topic: Mica Powders
- Replies: 16
- Views: 22392
Re: Mica Powders
Haley, I didn't test any TKB whites, only Pearlex. see my photo, 2nd row, last 3. Macro Pearl came out a medium sparkly silver, Micro Pearl came out white, and Pearl White came out a light silver.
- Fri Apr 12, 2013 2:46 pm
- Forum: Jewelry Making
- Topic: earring hooks
- Replies: 11
- Views: 46808
Re: earring hooks
cheapest is not best for earring hooks. unless the design is very small or light I always use 20 gauge sterling. I like the ones from FMG but you have to buy a lot to get the best pricing.