Search found 91 matches

by lorimendenhall
Thu May 01, 2014 1:58 pm
Forum: Techniques and Tools
Topic: Mica powders
Replies: 18
Views: 21774

Re: Mica powders

If anyone wants a copy of my mica test results pls email me at lorimendenhall @ cox.net
by lorimendenhall
Thu May 01, 2014 1:53 pm
Forum: Techniques and Tools
Topic: Bending 2mm Stringer
Replies: 12
Views: 14576

Re: Bending 2mm Stringer

oooh I like that word. never heard it before.
by lorimendenhall
Wed Apr 30, 2014 1:59 am
Forum: Jewelry Making
Topic: Can you recommend a great jewelry book for a newbie?
Replies: 4
Views: 34316

Re: Can you recommend a great jewelry book for a newbie?

Art Jewelry Magazine would be a good place to start.
by lorimendenhall
Wed Apr 30, 2014 1:58 am
Forum: Jewelry Making
Topic: belt buckle blanks
Replies: 5
Views: 34983

Re: belt buckle blanks

there are tons here: http://www.hhhenterprises.com/
by lorimendenhall
Mon Mar 24, 2014 6:04 pm
Forum: Techniques and Tools
Topic: silver and glass
Replies: 3
Views: 5598

Re: silver and glass

if you use fine silver it will stay bright silver colored. if you use sterling silver it turns ugly. I embed fine silver hangers into pendants all the time.
by lorimendenhall
Tue Mar 11, 2014 3:59 pm
Forum: Newcomer Forum
Topic: Searching for 4 pound containers of system 96 frit
Replies: 12
Views: 17136

Re: Searching for 4 pound containers of system 96 frit

I'd ask Spectrum who their resellers are. they will be glad to help you buy their product!
by lorimendenhall
Thu Feb 20, 2014 2:45 pm
Forum: Newcomer Forum
Topic: Can you recommend a glass grinder for a newbie?
Replies: 7
Views: 10621

Re: Can you recommend a glass grinder for a newbie?

I am a relative newbie. Bought a Gryphette and it meets my basic grinding needs, but I don't grind much... the price is low and it does the job.
by lorimendenhall
Wed Feb 12, 2014 9:58 pm
Forum: Newcomer Forum
Topic: Does this fusing mold need air holes?
Replies: 9
Views: 13727

Re: Does this fusing mold need air holes?

I doubt it needs holes. I full fuse onto a texture plate and there are no holes and it's fine. Also, I've got plenty of shallow slump molds that don't have holes.
by lorimendenhall
Tue Feb 04, 2014 3:38 pm
Forum: Newcomer Forum
Topic: Glassline Paper - need advice about hold time
Replies: 12
Views: 14868

Re: Glassline Paper - need advice about hold time

Kevin, you made a good point and I hadn't even thought of that. anywho my glass came out perfectly - no bubbles!
by lorimendenhall
Mon Feb 03, 2014 7:00 pm
Forum: Newcomer Forum
Topic: Glassline Paper - need advice about hold time
Replies: 12
Views: 14868

Re: Glassline Paper - need advice about hold time

they recommended 960 which was the old recommendation for annealing. now that the updated recommendation is 900 I adjusted. that's why I mentioned that the instructions were old : )
by lorimendenhall
Mon Feb 03, 2014 3:23 pm
Forum: Newcomer Forum
Topic: Glassline Paper - need advice about hold time
Replies: 12
Views: 14868

Re: Glassline Paper - need advice about hold time

thanks Brad and James. I did use little chads in the corners as they recommend. I'll know how it worked out tonight.
just fyi, here is what the directions said, except I changed their 960 to 900 (old directions!)
250/1000/4h
250/1470/15m
999/900/1h
250/200/0
by lorimendenhall
Mon Feb 03, 2014 12:23 am
Forum: Newcomer Forum
Topic: Glassline Paper - need advice about hold time
Replies: 12
Views: 14868

Re: Glassline Paper - need advice about hold time

I decided to just go with the instructions and just set it up with the 4 hour hold.
by lorimendenhall
Sat Feb 01, 2014 12:49 pm
Forum: Newcomer Forum
Topic: Glassline Paper - need advice about hold time
Replies: 12
Views: 14868

Glassline Paper - need advice about hold time

the directions say to hold at 1000 for 4 hours. that seems like a very long time. my piece is 6.5" square. how long would you bubble squeeze it for? also, will the other pieces in my kiln load be ok with that kind of soak? or is 4 hours perfectly normal and acceptable?
by lorimendenhall
Mon Jan 20, 2014 3:05 pm
Forum: Newcomer Forum
Topic: Slump Fail
Replies: 9
Views: 11477

Re: Slump Fail

agreed it's a tricky mold. I have that mold and the 2 times I used it were not successful. my issue both times was an air bubble in the center probably caused by holding too long and letting the air under there heat up rather than escape. besides the bubble in the center the sides were perfect!
by lorimendenhall
Sun Jan 19, 2014 2:52 pm
Forum: Kiln Casting
Topic: Making bisque ceramic molds
Replies: 8
Views: 14720

Re: Making bisque ceramic molds

you are right, top temp is 1700... that's too bad... thanks for the info.
by lorimendenhall
Sat Jan 18, 2014 12:48 pm
Forum: Kiln Casting
Topic: Making bisque ceramic molds
Replies: 8
Views: 14720

Re: Making bisque ceramic molds

what schedule would you use to bisque fire? I would like to make some textures. can I fire in my glass kiln? that would open up a whole new world!!!
by lorimendenhall
Thu Jan 16, 2014 7:49 pm
Forum: Business Topics
Topic: anybody in near orange ca?
Replies: 2
Views: 5941

Re: anybody in near orange ca?

I am probably going.
by lorimendenhall
Wed Jan 08, 2014 12:32 pm
Forum: Newcomer Forum
Topic: Sticky cabochons: shelf paper vs kiln wash again
Replies: 24
Views: 30344

Re: Sticky cabochons: shelf paper vs kiln wash again

maybe try a different brand of kiln wash. I use Hotline Primo and have this problem a lot too. people have told me this brand does that.
by lorimendenhall
Sat Jan 04, 2014 2:02 pm
Forum: Newcomer Forum
Topic: New
Replies: 12
Views: 14933

Re: New

a couple of you mentioned how much you love the window... please help newbie... I can't see jack through my window. it's too small and there is no light in the kiln for much of the time. do you shine a flashlight into the window so you can see anything. my window was a waste of $60.
by lorimendenhall
Fri Jan 03, 2014 7:00 pm
Forum: Techniques and Tools
Topic: Sandblaster or WBS?
Replies: 7
Views: 9945

Re: Sandblaster or WBS?

but a sandblaster is so fun!!!! I actually want both of these things too...