Search found 4 matches

by Shirley Bishop
Thu Jul 11, 2013 12:39 pm
Forum: Techniques and Tools
Topic: Using Photo Fusing Paper for the first time
Replies: 9
Views: 20977

Re: Using Photo Fusing Paper for the first time

Thanks everyone for your replies. I am happy to announce that my brother has a HP5100 that worked beautifully! It does take some searching but you can find the MSDS sheets on either Canon or HP sites to check their toner cartridges for the iron oxide. This one said less than 50 but it worked great! ...
by Shirley Bishop
Thu Jul 04, 2013 3:37 pm
Forum: Techniques and Tools
Topic: Using Photo Fusing Paper for the first time
Replies: 9
Views: 20977

Using Photo Fusing Paper for the first time

I'm somewhat new to fusing but want to try Fusing Photo Paper that i ordered from Delphi. My question is the printer and toner. I asked a guy at the Office Depot who told me he could not find anything on the internet on a MSDS sheet for the Canon toner that showed the toner contains IRON OXIDE like ...
by Shirley Bishop
Tue May 14, 2013 1:53 pm
Forum: Newcomer Forum
Topic: Workbench?
Replies: 20
Views: 60547

Workbench?

My husband wants to build me a workbench. He would like some suggestions or better yet pictures of what works for you. I used a great one in a class that was about 34" deep (work surface) and about 6 foot long. But we don't know how high it was. It was also on wheels. It had metal legs and wood...
by Shirley Bishop
Mon Apr 29, 2013 9:41 am
Forum: Newcomer Forum
Topic: Cracked :(
Replies: 3
Views: 9587

Cracked :(

Newbie here. I just fired a 11 x 8 platter. 6mm of base with deco pieces on top and a bit of frit. Came out beautiful but i was too anxious and took it out at 200 degrees instead of waiting for it to totally cool. Then to make matters worse i stuck it under some warm water to clean off the fired she...