How many hobbyists own a kiln?
Does anyone have an idea of how many glass hobbyists own a kiln? In the US? Or English speaking countries? Or, world wide?
- Tue Apr 30, 2013 6:43 pm
- Forum: Jewelry Making
- Topic: High temperature wire between glass
- Replies: 3
- Views: 13222
High temperature wire between glass
I have been trying to place a small wire ring between two layers of glass, prior to firing. The ring is made out of high temperature wire and will attach directly to the earring finding instead of using a glued on bail. The problem I have is that the high temperature wire becomes tarnished and britt...