Search found 579 matches
- Sat Sep 12, 2015 9:26 pm
- Forum: Techniques and Tools
- Topic: Glass seperator an Colour DeVerre molds
- Replies: 2
- Views: 5411
Re: Glass seperator an Colour DeVerre molds
I'd send your questions directly to the manufacturer. They're very helpful and responsive.
- Wed Sep 02, 2015 10:54 pm
- Forum: Newcomer Forum
- Topic: Need help with Creative Ceramics medium rectangle mold
- Replies: 15
- Views: 27166
Re: Need help with Creative Ceramics medium rectangle mold
Have to agree with Don. Without seeing your mold, it appears that as the glass slumped, it trapped air which caused the bubble.
- Sun Aug 30, 2015 5:29 pm
- Forum: Newcomer Forum
- Topic: Pre-firing Stringers
- Replies: 6
- Views: 13377
Re: Pre-firing Stringers
I guess you'd have to test for your kiln, but when I slump stringer, I fire afap to 1250° and hold until visually confirmed. If you're trying for a flat side, you'd probably have to fire a little hotter. I'd choose a temp to start with and monitor them. When they should be done, quickly remove one w...
- Sat Aug 29, 2015 10:33 pm
- Forum: Techniques and Tools
- Topic: Getting cerium oxide out of small bubbles.
- Replies: 5
- Views: 9075
Re: Getting cerium oxide out of small bubbles.
Buy an old Water Pik at a thrift store. Mini water jet!
- Fri Aug 28, 2015 6:39 pm
- Forum: Techniques and Tools
- Topic: Irid
- Replies: 5
- Views: 8624
Re: Irid
AAE Glass is selling a product called Glass Glo paints. They appear to be a dry mica cake that you can wet with water or other mediums. There's a video right now showing that they product an irid-like coating. The nice thing is, they're mixable. https://www.aaeglass.com/catalogsearch/result/?cat=0&a...
- Tue Aug 25, 2015 2:38 pm
- Forum: Techniques and Tools
- Topic: Airbrushing Problems with Bullseye Color Line
- Replies: 6
- Views: 10517
Re: Airbrushing Problems with Bullseye Color Line
Thanks for that, Carol! Obviously, I misunderstood.
I always fire my kilns with the peep holes open during the entire firing, so haven't noticed any difference with the reds. I haven't worked with Colorline extensively, though.
Here's my test piece:
I always fire my kilns with the peep holes open during the entire firing, so haven't noticed any difference with the reds. I haven't worked with Colorline extensively, though.
Here's my test piece:
- Mon Aug 24, 2015 8:10 pm
- Forum: Techniques and Tools
- Topic: Airbrushing Problems with Bullseye Color Line
- Replies: 6
- Views: 10517
Re: Airbrushing Problems with Bullseye Color Line
Linda, I'm not sure what you mean. When I click on that link, it takes me to Colorline's pdf instruction book. If the link is giving you a warning, you may just want to do a Google search for their site.
- Mon Aug 17, 2015 1:04 pm
- Forum: Techniques and Tools
- Topic: Airbrushing Problems with Bullseye Color Line
- Replies: 6
- Views: 10517
Re: Airbrushing Problems with Bullseye Color Line
In my test samples, thicker applications would tend to crackle a bit.
How fast/hot are you firing?
Here are the instructions:
http://www.colorlinepaints.com/pdf/colo ... let-en.pdf
How fast/hot are you firing?
Here are the instructions:
http://www.colorlinepaints.com/pdf/colo ... let-en.pdf
- Thu Aug 13, 2015 1:03 pm
- Forum: Jewelry Making
- Topic: ripple dichro - how to cap without bubbles?
- Replies: 10
- Views: 49626
Re: ripple dichro - how to cap without bubbles?
I make sure to press firmly with my cutter when cutting thicker glass, and always dip in cutting oil first. It takes a bit more strength to squeeze my running pliers for thicker glass. I have heavy duty running pliers but don't use them; they've got metal jaws which aren't covered with rubber, so I ...
- Mon Aug 03, 2015 1:08 pm
- Forum: Techniques and Tools
- Topic: soap dish/molds
- Replies: 16
- Views: 19924
Re: soap dish/molds
If you slow those ramps down, your glass will experience more heatwork and less funky stretching. Think of gently guiding the glass into the mold. I slump at 250° per hour. There's no reason for your hold at 1100°.
- Mon Aug 03, 2015 1:03 pm
- Forum: Jewelry Making
- Topic: ripple dichro - how to cap without bubbles?
- Replies: 10
- Views: 49626
Re: ripple dichro - how to cap without bubbles?
When I was making lots of jewelry from larger tiles, I always cut them by hand. You easily cut 2-3 layers and with a little more effort 4 layers by hand. Since you're grinding and fire polishing anyway, it makes it much faster than dragging out the saw.
- Fri Jul 31, 2015 12:37 pm
- Forum: Jewelry Making
- Topic: ripple dichro - how to cap without bubbles?
- Replies: 10
- Views: 49626
Re: ripple dichro - how to cap without bubbles?
When I was doing jewelry with rippled dichro, I'd make larger tiles to cut down. A 6x6" piece in my kilns, with a clear cap, would look something like this: 300° to 1150°, no hold 50° to 1250°, hold 60 300° to 1440°, hold 15 (or until visually confirmed) full to 900°, hold 60 I have several kil...
- Wed Jul 15, 2015 7:25 pm
- Forum: Techniques and Tools
- Topic: marking glass to be cut with Revolution XT
- Replies: 13
- Views: 18958
Re: marking glass to be cut with Revolution XT
I know someone who used to stick her paper patterns on with a light coating of rubber cement.
- Sat Jul 11, 2015 11:17 pm
- Forum: Techniques and Tools
- Topic: Second fuse??
- Replies: 4
- Views: 6573
Re: Second fuse??
Some dichroic glass is just rougher after being fired. Some will splinter and tiny pieces will pop off and deposit elsewhere on your glass. Some fires satiny smooth. Some crackles. My guess is you've got glass from different manufacturers and different coatings. I see that a few of your sizzle stick...
- Wed Jul 01, 2015 12:36 am
- Forum: Techniques and Tools
- Topic: Kiln running when it's over 95 outside
- Replies: 4
- Views: 8058
Re: Kiln running when it's over 95 outside
We hit 100° today. I ran two of my kilns simultaneously. Now and then we'll have brownouts if everyone's running their AC but hasn't happened this year.
- Tue Jun 30, 2015 12:07 am
- Forum: Techniques and Tools
- Topic: MR97 problems HELP
- Replies: 3
- Views: 6131
Re: MR97 problems HELP
I've have limited knowledge of MR-97 but the few times I used it I had the same problem. Turns out, it's from too much sprayed on.
I wasn't able to remove the haze, and I tried everything. Wound up sandblasting.
I wasn't able to remove the haze, and I tried everything. Wound up sandblasting.
- Fri Jun 26, 2015 11:40 am
- Forum: Techniques and Tools
- Topic: Skutt GM1014 - Can Handles Be Used to Lift?
- Replies: 4
- Views: 7898
Re: Skutt GM1014 - Can Handles Be Used to Lift?
My Skutt GM1414 is over 300 pounds; we used the four handles to lift, carry, and level it.
- Fri Jun 26, 2015 11:39 am
- Forum: Techniques and Tools
- Topic: Hanging Panels
- Replies: 3
- Views: 6042
Re: Hanging Panels
I use those Panelclips too. On smaller pieces, I use 3M VHB (very high bond) tape.
- Sun Jun 21, 2015 11:20 pm
- Forum: Techniques and Tools
- Topic: spray kiln shelf
- Replies: 6
- Views: 12016
Re: spray kiln shelf
I've done several things over the years, trying to find the easiest way to deal with shelves. First, I used a paint roller to apply wash. After dry, I'd lightly 'sand' it with a piece of smooth printer paper. Then, I used the garden sprayer approach. That leaves fairly large blobs and splatters, so ...
- Fri Jun 19, 2015 11:37 am
- Forum: Techniques and Tools
- Topic: Mixing liquid enamels with powedrs
- Replies: 19
- Views: 28217
Re: Mixing liquid enamels with powedrs
I believe adding flux is what you should do.