Search found 958 matches
- Thu Mar 13, 2014 10:32 am
- Forum: Community Projects
- Topic: Mailing magnets
- Replies: 8
- Views: 38279
Re: Mailing magnets
micheals
- Fri Mar 07, 2014 9:55 pm
- Forum: Techniques and Tools
- Topic: Kiln cement for chipped brick
- Replies: 2
- Views: 4907
Re: Kiln cement for chipped brick
what harm does leaving the chips do?
- Thu Mar 06, 2014 11:25 pm
- Forum: Techniques and Tools
- Topic: Lid Element replacement
- Replies: 4
- Views: 7303
Re: Lid Element replacement
if you have a gfi on it that is tripping, then you've mis-wired it and there's a short to ground somewhere. look for an element wire that is touching the metal shell somewhere.
- Tue Mar 04, 2014 9:43 pm
- Forum: Techniques and Tools
- Topic: firing problem
- Replies: 23
- Views: 23970
Re: firing problem
you're confusing volts and amps.if you talk to your electrician like that, he's either going to be confused, or will have to teach you. it pulls amps (consumes electricity). that is what the kiln maker can control (by the element size). it is powered with volts, and the kiln maker doesn't have any c...
- Tue Mar 04, 2014 1:21 am
- Forum: Techniques and Tools
- Topic: firing problem
- Replies: 23
- Views: 23970
Re: firing problem
they're pulling your leg. fth is failure to heat fast enough. this means there either isn't enough power, or enough elements. adding more insulation to the sides will prevent heat escaping, which may help it heat up faster, but paper won't do anything because once the binder is burned off, there's n...
- Wed Feb 26, 2014 9:52 pm
- Forum: Newcomer Forum
- Topic: Making channels with fiber paper
- Replies: 8
- Views: 10712
Re: Making channels with fiber paper
i use thin braided wire to hang chimes. it lasts far longer in the sun.
- Wed Feb 26, 2014 1:13 am
- Forum: Techniques and Tools
- Topic: Gloves for Cyclone 3824
- Replies: 8
- Views: 12089
Re: Gloves for Cyclone 3824
http://www.harborfreight.com/oil-resistant-pvc-long-cuff-gloves-99677.html http://www.harborfreight.com/rubber-blasting-gloves-4468.html http://www.amazon.com/Rubber-Gloves-Sandblast-Cabinet-Gallon/dp/B004UC6O22 there's lots of replacement gloves. when i built my cabinet, i just got a pair of replac...
- Sun Feb 23, 2014 10:52 pm
- Forum: Techniques and Tools
- Topic: Kilns
- Replies: 24
- Views: 62056
Re: Kilns
[quote="Jeanne"]@ Bobbie - Per your original post... You said your kiln is 12 years old and you fire it daily - perhaps it's time to bid it adieu. The amount of time, effort and money you've spent/or may spend, to rehabilitate this kiln sounds like a lot, (are you still using the original ...
- Sun Feb 23, 2014 10:51 pm
- Forum: Techniques and Tools
- Topic: MK -100 saw water source
- Replies: 10
- Views: 13824
Re: MK -100 saw water source
[quote="S.TImmerman"]Thank you all for the replies, nasty flu got me. Charlie I suspect much of it from our golden retriever who is constantly by my side AND that bucket. They shed like mad. Plus our 17 year old rescue Persian and very deaf, he'd sit in the tray for the saw if I let him. T...
- Sun Feb 23, 2014 10:50 pm
- Forum: Techniques and Tools
- Topic: How to make SURE my electric works before buying kiln?
- Replies: 11
- Views: 10535
Re: How to make SURE my electric works before buying kiln?
if you're not able to look in the breaker box and answer these questions, then you need an electrician. it would be too dangerous for us to guess what you have.
- Mon Feb 17, 2014 1:35 am
- Forum: Newcomer Forum
- Topic: Drape stupid glass, drape, please
- Replies: 3
- Views: 4787
Re: Drape stupid glass, drape, please
small things slump or drape slower and take more heat work to look the same as large ones. there's not much weight in the glass at the end of the tips to pull it down. the glass has to be more fluid to move. you have fiber paper under it, which could be holding it up somewhat too, although it's pret...
- Mon Feb 17, 2014 1:33 am
- Forum: Techniques and Tools
- Topic: MK -100 saw water source
- Replies: 10
- Views: 13824
Re: MK -100 saw water source
i don't understand. if the pump is in fresh water all the time, where is the glass dust coming from? do you have the water draining from the hole in the tray back into the bucket, or where does it go? if it is getting into the pump bucket, you might try making a cascade bucket line, and put the pump...
- Mon Feb 17, 2014 12:05 am
- Forum: Newcomer Forum
- Topic: Drape stupid glass, drape, please
- Replies: 3
- Views: 4787
Re: Drape stupid glass, drape, please
you need to turn your kiln upside down. it looks like it's trying to drape up.
- Mon Feb 17, 2014 12:03 am
- Forum: Techniques and Tools
- Topic: MK -100 saw water source
- Replies: 10
- Views: 13824
Re: MK -100 saw water source
and what are the plugs consist of, and where is that coming from?
- Sun Feb 16, 2014 1:47 pm
- Forum: Newcomer Forum
- Topic: How did this happen?
- Replies: 11
- Views: 31559
Re: How did this happen?
[quote="Shelley Lewis"]Dana,
Two layers plus a little frit on top
[/quote]
well, i guess it does need holes. the bubbles came from trapped air. if you get the glass off, note where the bubbles where, and drill small holes there (and perhaps elsewhere in the swirl).
Two layers plus a little frit on top
[/quote]
well, i guess it does need holes. the bubbles came from trapped air. if you get the glass off, note where the bubbles where, and drill small holes there (and perhaps elsewhere in the swirl).
- Sun Feb 16, 2014 12:17 pm
- Forum: Newcomer Forum
- Topic: How did this happen?
- Replies: 11
- Views: 31559
Re: How did this happen?
if it's mechanically held (by the swirls probably or a slight undercut, turn it upside down and suspend from 1" posts on the edges of the mold only. slowly heat up to annealing temp as a top temp, and listen. if it's not fused to the mold, it should drop off sometime before you get to 1000.
- Sat Feb 15, 2014 11:42 am
- Forum: Newcomer Forum
- Topic: drapeing 9in. single sheet over SS bowl
- Replies: 12
- Views: 15445
Re: drapeing 9in. single sheet over SS bowl
[quote="wharrel"]I forgot to state that I had put a 1/32 fiber sheet on top of the SS because I thought the SS was heating up faster than the glass and causing a hotspot where the glass touched the SS. Thanks to all for the help. I will take out the kiln posts and shelves and ramp at 150 u...
- Fri Jan 24, 2014 8:04 pm
- Forum: Newcomer Forum
- Topic: Sticky cabochons: shelf paper vs kiln wash again
- Replies: 24
- Views: 30317
Re: Sticky cabochons: shelf paper vs kiln wash again
[quote="Morganica"]I do much the same thing with plaster of paris. I tend to use a broad spackling knife to flatten mine, but a rolling pin is a cool idea.[/quote]
i use a wine bottle with the neck cut off. no handles on the ends to run into the kiln walls.
i use a wine bottle with the neck cut off. no handles on the ends to run into the kiln walls.
- Wed Jan 22, 2014 11:00 pm
- Forum: Techniques and Tools
- Topic: hire fire glue?
- Replies: 2
- Views: 4212
Re: hire fire glue?
i doubt it. most glues are organic, and organics can't usually last that high. there may be some hi-temp epoxies; for instance, you can use some epoxies on car headers, which probably reach 800-900F or so.
- Sun Jan 19, 2014 2:25 am
- Forum: Techniques and Tools
- Topic: Spectrum label "ghost"
- Replies: 18
- Views: 18554
Re: Spectrum label "ghost"
[quote="Cheryl Maahs"][quote="Andrea R"][quote="Cheryl Maahs"]I use WD40 to remove the "residue", then nail polish remover[/quote] Seems like a lot of work to get a label off :shock:[/quote] Maybe ... But ... WD40 is fish oil and behaves like Goo Gone and the ...