by rosanna gusler
Sat Jul 19, 2003 5:59 am
Forum: Kiln Casting
Topic: spray foam
Replies: 9
Views: 8402

i would think that barring undercuts the foam could stay as one with the latex. otherwise a good coating of spray grease would probably work fine. i am putting this idea into my 'to try' file. rosanna
by rosanna gusler
Thu Jul 17, 2003 6:53 am
Forum: Kiln Casting
Topic: spray foam
Replies: 9
Views: 8402

spray foam

i wonder if the spray foam greg was talking about in another thread would make a good backing to stiffen up a cured latex mold. put it on before the mold is removed. rosanna
by rosanna gusler
Wed Jul 16, 2003 4:23 pm
Forum: Kiln Casting
Topic: release agent for between plaster
Replies: 7
Views: 7278

murphys oil soap works for me. maybe you will want to pull a latex type mold off your origonal so you can duplicate it if it gets damaged. rosanna
by rosanna gusler
Sun Jul 13, 2003 8:33 am
Forum: Business Topics
Topic: holiday studio tour Q?
Replies: 8
Views: 6583

marty, you are too funny! 1$ ! i will throw this idea out as well. thanks. rosanna
by rosanna gusler
Sun Jul 13, 2003 7:01 am
Forum: Techniques and Tools
Topic: yellow discolouration in float glass
Replies: 8
Views: 5019

any chance that there can be some form of silver in your silica? silver foil, silver filings, stirring with a silver spoon? rosanna
by rosanna gusler
Sat Jul 12, 2003 12:34 pm
Forum: Business Topics
Topic: holiday studio tour Q?
Replies: 8
Views: 6583

ok, that is a start. we are a diverse group, potters, weaver carver, painters,me.......... priobably about 15-20. last year we thought about this in october. MAYBE , starting now we can pull this together. rosanna
by rosanna gusler
Sat Jul 12, 2003 8:09 am
Forum: Business Topics
Topic: holiday studio tour Q?
Replies: 8
Views: 6583

holiday studio tour Q?

hi all, we artists on roanoke island are beginning to organise our first annual (we hope) pre christmas studio tour. any of you have any helpful hints/ideas to do (or avoid)? thanks, rosanna
by rosanna gusler
Thu Jul 10, 2003 8:58 am
Forum: Techniques and Tools
Topic: Drape question
Replies: 5
Views: 4019

not stewart but, regular black iron pipe. NOT galvanized. also steel bolts with a large fender washer and a nut under that. i put a piece of fiber on top. rosanna
by rosanna gusler
Tue Jul 08, 2003 7:03 am
Forum: Techniques and Tools
Topic: plaster molds
Replies: 1
Views: 1996

hi bonnie, there is a thread going on molds in kiln casting dept right now that has good info. also search molds in the archives old and new. rosanna
by rosanna gusler
Tue Jul 08, 2003 6:55 am
Forum: Techniques and Tools
Topic: confused about adhesive for mirror
Replies: 12
Views: 28961

i wonder if the 'neutral cure' silicones would be safer? they do not have that acrid oder. rosanna
by rosanna gusler
Mon Jul 07, 2003 9:58 am
Forum: Techniques and Tools
Topic: Tips and Tricks
Replies: 15
Views: 10282

i just really have a problem believing that there is any water left in a shelf at softening temps. i put wet shelves in the kiln alot. no problems. rosanna
by rosanna gusler
Mon Jul 07, 2003 9:54 am
Forum: Techniques and Tools
Topic: Warmies in Richmond, VA?
Replies: 2
Views: 2480

not from richmond but that sounds exciting enough to come see! not a long trip from the obx. rosanna
by rosanna gusler
Sun Jul 06, 2003 8:48 pm
Forum: Techniques and Tools
Topic: frit chips and elmer's Q
Replies: 2
Views: 2470

and you are the man for frit controll! had another house guest go through this years mags and pick the orange tree as sumpin special!! rosanna
by rosanna gusler
Thu Jun 26, 2003 6:55 am
Forum: Business Topics
Topic: foreign magazines/books
Replies: 3
Views: 4069

sounds kind of strange. there are some internet scams that target artisits going around now. i wonder about that 'competition' in korea. can't think of the name of it right now but it has full page ads in 'artist calander' mag and 'crafts report' too i think. 20 k prize i think. i just wonder how ma...
by rosanna gusler
Tue Jun 24, 2003 8:35 am
Forum: Techniques and Tools
Topic: magless article in artglass info
Replies: 0
Views: 2040

magless article in artglass info

wow! what a great article. it brought back all the fun of the event to me. great job barbara! thanks again beth et al for all the hard work bringing this together. rosanna
by rosanna gusler
Sun Jun 22, 2003 2:32 pm
Forum: Techniques and Tools
Topic: Glass crushers
Replies: 14
Views: 8615

hi marge, there are several good threads about do it yourself in the archives old and new. some with photos. i can not remember their titles though. rosanna ps also look up quenched frit while you search
by rosanna gusler
Wed Jun 18, 2003 1:12 pm
Forum: Techniques and Tools
Topic: Buying float glass
Replies: 14
Views: 9766

hi john, i have been having some problems with edges as well. not devit so much as little fissures or cracks on fuse. i wet sand these out for the slump and the edges fire polish out nicely. i did have devit problems and got rid of those by religiously cleaning the cut edge. you would think that it ...
by rosanna gusler
Mon Jun 16, 2003 7:23 am
Forum: Photos and Stuff
Topic: New studio, new work.
Replies: 6
Views: 5870

wow! that 'sky' in waterhole series is amazing. what a sense of largeness. rosanna
by rosanna gusler
Mon Jun 16, 2003 6:27 am
Forum: Kiln Casting
Topic: Casting kiln
Replies: 8
Views: 8300

so who's the manufacturer? rosanna
by rosanna gusler
Sun Jun 15, 2003 10:06 am
Forum: Techniques and Tools
Topic: Attaching zinc or brass channel to picture frame
Replies: 3
Views: 3191

another casual loop trick is to lamp work some glass strips into rings or U's and fuse those where needed for hangers. i make a double ring to get the glass to the preferred thickness. rosanna