I'm finding some of my necklace bales and ring settings are not sealing right. especially if they get wet.
I've cured them. for 7 days but maybe 20 percent fall apart
would it help if the glass is perfectly smooth. my kiln paper has slight impression
glue on bales
Moderators: Brad Walker, Tony Smith
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: glue on bales
What are you using as an adhesive?
A smooth surface is not what you want to adhere to.
I have a tutorial on my site (see below) about adhering bails.
Barry
A smooth surface is not what you want to adhere to.
I have a tutorial on my site (see below) about adhering bails.
Barry
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: glue on bales
I use a small diamond grinder bit to roughen up contact surface on glass and sand bale to remove production lubricants.. then use E6000 NEVER FAILS!!
"The Glassman"
-
Michael Stevens
- Posts: 83
- Joined: Thu Dec 26, 2019 2:52 pm
Re: glue on bales
I use e6000, but perhaps I don't seal it evenly on some pieces, or too thick. but I didn't think about the oils on the bale. but I'll spend more time grinding the surface a little. I have some that feel quite strong and others that pop off easily
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: glue on bales
If you look at the failures, you will see that one or the other of the attached pieces has all the adhesive. The other one is improperly prepared.
Again, check my tutorial. It explains it all.
Again, check my tutorial. It explains it all.
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
-
Michael Stevens
- Posts: 83
- Joined: Thu Dec 26, 2019 2:52 pm
Re: glue on bales
thanks, unfortunately can't see your tutorial it's blocked here I don't use a vpn, so I'm limited on what to see. but that's ok. I think it will be ok now.