okay so I got the shape I want with the grinder but now..

Post here with questions and topics relating to making glass jewelry.

Moderators: Brad Walker, Tony Smith

Post Reply
grayeye
Posts: 7
Joined: Fri Mar 14, 2014 11:21 pm

okay so I got the shape I want with the grinder but now..

Post by grayeye »

I used a glass grinder to shape the pieces because they looked like blobs (after using a microwave kiln) but now the edges are ugly mat black. now what?
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: okay so I got the shape I want with the grinder but now.

Post by Stephen Richard »

Grind with successively fine sandpaper or diamond pads and water until a luster, then fire polish
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
grayeye
Posts: 7
Joined: Fri Mar 14, 2014 11:21 pm

Re: okay so I got the shape I want with the grinder but now.

Post by grayeye »

Thank you.
What is firepolish? and how do I do it?
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: okay so I got the shape I want with the grinder but now.

Post by Stephen Richard »

Look at the tutorial on the main site www.warmglass.com
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/