domed pendant

Post here with questions and topics relating to making glass jewelry.

Moderators: Brad Walker, Tony Smith

Post Reply
eclairewl
Posts: 3
Joined: Mon Apr 26, 2004 4:47 pm
Location: Wilmington, DE
Contact:

domed pendant

Post by eclairewl »

I bought a pendant in Spain that was a domed circle and I have been trying to figure out how to do this.
Any ideas?
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: domed pendant

Post by Judd »

A glass dome?
Well, you could make a circle, then slump it in a dome shaped mold.
eclairewl
Posts: 3
Joined: Mon Apr 26, 2004 4:47 pm
Location: Wilmington, DE
Contact:

Re: domed pendant

Post by eclairewl »

These are 1 inch circles with a convex suface. I am going to give it a try making my round pendant flat and using a slightly larger piece of glass over it. I do this for small earrings but haven't tried it for larger pieces.
Glass Fever
Posts: 29
Joined: Sat Aug 04, 2007 11:08 pm
Location: Chicago Suburbs
Contact:

Re: domed pendant

Post by Glass Fever »

Are you sure it was fused and not torch worked? There are small casting molds available that may give you the look you're after.
eclairewl
Posts: 3
Joined: Mon Apr 26, 2004 4:47 pm
Location: Wilmington, DE
Contact:

Re: domed pendant

Post by eclairewl »

It was definitely fused but I think I finally figured out how it was done: by heating the 2 pieces to 1500 I was able to achieve the effect.
Thanks for your help.