The right torch for bullseye rods
Moderators: Tony Smith, Brad Walker
-
- Posts: 38
- Joined: Tue Nov 06, 2007 10:16 am
The right torch for bullseye rods
I tried to make little leaves using bullseye rods. I used a dual-fuel torch (oxygen and propane), but the glass colors changed and the clear glass rod turned greyish. Is a single fuel torch better with soft glass ?
-
- Posts: 187
- Joined: Mon Mar 10, 2003 11:44 am
- Location: eastern Tennessee
- Contact:
Re: The right torch for bullseye rods
Dual is required, but it must be surface mix, not premix. I've been using a Nortel minor for many years and now have switched to a Bethlehem Alpha, You also have to have your flame adjusted correctly and work way out in the end of the flame.
-
- Posts: 38
- Joined: Tue Nov 06, 2007 10:16 am
Re: The right torch for bullseye rods
Many thanks Tom
-
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: The right torch for bullseye rods
Main thing is to use the proper gas mix, and work way out in the flame.
-
- Posts: 38
- Joined: Tue Nov 06, 2007 10:16 am
Re: The right torch for bullseye rods
Thank you for your tip Jim