2013 Magnet Exchange How Tos

This is the forum for discussing Warm Glass community projects such as the Magnet Exchange, the Collaboration, and similar efforts.

Moderator: Tony Smith

Post Reply
Jennifer Polver
Posts: 37
Joined: Thu May 31, 2007 10:31 pm
Location: Alpharetta, GA
Contact:

2013 Magnet Exchange How Tos

Post by Jennifer Polver »

Here are the how tos http://warmglass.com/magnet/2013%20Magn ... 040113.pdf

Brad, thanks for uploading the file
RachelM
Posts: 47
Joined: Mon Oct 24, 2011 11:26 pm

Re: 2013 Magnet Exchange How Tos

Post by RachelM »

THANK YOU THANK YOU THANK YOU!
=D> =D> =D> =D> =D> =D> =D> =D>

I have been checking every few hours waiting for THIS!
Just ready through it very quickly and now will print out and take home to read before bedtime....like a good murder-mystery novel!

Many thanks to you and Susan and Brad for the 2013 Magless Exchange!

Rachel
imaglassydiva@aol.com
KaCe
Posts: 126
Joined: Sun May 15, 2005 2:25 pm
Location: Old Town, Tacoma, WA
Contact:

Re: 2013 Magnet Exchange How Tos

Post by KaCe »

Thank you to all who worked so hard on this year's exchange. I appreciate that it kicks me in the buttocks and helps me clear my mind and do something outside my usual. I am not very prolific and so making 50 of anything is more production than I usually do. I LOVE getting the box filled with charming, stunning, ingenious and inspiring maglesses. Thank you everyone.

KaCe
haleybach
Posts: 75
Joined: Tue Sep 04, 2012 1:59 pm
Location: Austin TX

Re: 2013 Magnet Exchange How Tos

Post by haleybach »

Thanks to Jennifer, you did a nice job putting the how to's together! I really like the photos at the top.

I have a question on #26 is all the color in the top layer from the Dense White/ French Vanilla reaction? Is that where the blue in the stenciled pattern is coming from?
Studiodunn
Posts: 106
Joined: Sun Sep 11, 2011 9:30 am
Location: The Dunn-Inn
Contact:

Re: 2013 Magnet Exchange How Tos

Post by Studiodunn »

Thank you Jennifer for taking ALL that time to sift through ALL those emails to compile the "How to's" for this years exchange. It was a pleasure participating!

After I submitted my "How to" description, I ended up making some subtle tweaks and posted about the experience on my blog for anyone who might be interested...

http://studiodunndesigns.wordpress.com/ ... -exchange/
“I would rather die than hate you.”
- Martin Luther King
charles r. hall
Posts: 6
Joined: Thu Feb 23, 2006 1:53 am
Location: Napa. Ca.

Re: 2013 Magnet Exchange How Tos

Post by charles r. hall »

I can't get this to open. It just seems to freeze the page. Any suggestions?
thanks
Charles Hall
"Keep your dreams as clean as silver" John Stewart 1939-2008
Jennifer Polver
Posts: 37
Joined: Thu May 31, 2007 10:31 pm
Location: Alpharetta, GA
Contact:

Re: 2013 Magnet Exchange How Tos

Post by Jennifer Polver »

Charles,

I just emailed you the PDF.

Jennifer
Dianne Van de Carr
Posts: 18
Joined: Sun Mar 09, 2003 3:43 pm
Location: Carmichael, CA
Contact:

Re: 2013 Magnet Exchange How Tos

Post by Dianne Van de Carr »


I have a question on #26 is all the color in the top layer from the Dense White/ French Vanilla reaction? Is that where the blue in the stenciled pattern is coming from?
It sure is. Only French Vanilla and Dense White were used and it took 2 firings for the reaction to develop.
Dianne
haleybach
Posts: 75
Joined: Tue Sep 04, 2012 1:59 pm
Location: Austin TX

Re: 2013 Magnet Exchange How Tos

Post by haleybach »

Dianne Van de Carr wrote:

I have a question on #26 is all the color in the top layer from the Dense White/ French Vanilla reaction? Is that where the blue in the stenciled pattern is coming from?
It sure is. Only French Vanilla and Dense White were used and it took 2 firings for the reaction to develop.
Dianne
Wow. Beautiful!
Post Reply