Hello everybody,
I discovered a nice pack of Uroboros glass in my storage.
Some of it is very nice colors.Eventhough its COE is 90 - it is fired on different schedule than BE.

Being weak in numbers, I would appreciate it if anybody could refer me to Uroboros firing schedule for SMOOSHED GLASS, or UNDER PRESSURE or [color=#BF40FF]KILN PRESSED GLASS[/color] - those are all names of the same process.

I'd be more than grateful!!!


Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com

Brad Walker
Site Admin
Posts: 1385
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Schedule for kiln pressed glass - for Uroboros

Postby Brad Walker » Sat Apr 24, 2021 9:02 pm

I never fired Uro 90 that much (if any) different than Bullseye. The same schedule ought to work.

Havi
Posts: 598
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Schedule for kiln pressed glass - for Uroboros

Postby Havi » Sun Apr 25, 2021 1:59 am

Thank, Brad

My best teacher!

Did you also mix BE AND URO????

many thanks in advance

H
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com

Brad Walker
Site Admin
Posts: 1385
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Schedule for kiln pressed glass - for Uroboros

Postby Brad Walker » Sun Apr 25, 2021 8:44 am

Havi wrote:Did you also mix BE AND URO????


Always the clear Uro with BE, no problems. Sometimes the other colors. Only problem I ever experienced was with one of the Uroboros reds. Not surprising since reds can be difficult to make.

Havi
Posts: 598
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Schedule for kiln pressed glass - for Uroboros

Postby Havi » Mon Apr 26, 2021 3:28 pm

Thanks a lot, Brad

Always appreciate your knowledge,
and
your
sharing it!!!

Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 27 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com