Hxtal and HYG adhesives - WarmGlass.com

Hxtal and HYG adhesives

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
flite risk
Posts: 4
Joined: Sat Mar 04, 2006 10:54 am
Location: Hamilton, MT

Hxtal and HYG adhesives

Postby flite risk » Tue Sep 14, 2021 1:41 pm

Hi all. I have always used mechanical means to attach my glass to other mediums but want to start using adhesives because I am hoping it creates new opportunities with my artwork. I have Hxtal, Hang Your Glass and E6000 in my shop. I looked through the archives and it seems that Hxtal had the least failures for most of the folks that chimed in. I am aware of it's long setup time and that doesn't bother me as I am more concerned with bond failure than time. I have used the HYG and it sure seems to work quick and create a strong bond although some folks mentioned it yellows after time...which doesn't bother me either because I would hide the bond. I did read that some folks had some failure with it over time...which I don't want and is why I have been reluctant to use adhesives. I would appreciate opinions from folks that have used adhesives to bond metal (aluminum) to glass and glass to glass. As an experiment I have already bonded (Hxtal) some heavy glass pieces to a thick aluminum sheet and will be hanging it up to see how it does. Any input appreciated! Thanks
SDG

Dick
Posts: 84
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: Hxtal and HYG adhesives

Postby Dick » Fri Sep 24, 2021 7:18 pm

Of the three I would only use hxtal and never the others. had problems with yellowing and failing. The only other I use, and I use it mostly for hanging hardware is loctite hysol h30cl. It is super for metal to glass, never yellows. Course if I have to cold work, it's back to hxtal

flite risk
Posts: 4
Joined: Sat Mar 04, 2006 10:54 am
Location: Hamilton, MT

Re: Hxtal and HYG adhesives

Postby flite risk » Tue Oct 26, 2021 6:41 pm

Dick wrote:Of the three I would only use hxtal and never the others. had problems with yellowing and failing. The only other I use, and I use it mostly for hanging hardware is loctite hysol h30cl. It is super for metal to glass, never yellows. Course if I have to cold work, it's back to hxtal

Thanks for the input. I have never heard of Loctite hysol h30cl so will look it up. Thats exactly what I am looking for to adhere the glass directly to the aluminum. Thanks!
SDG


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 31 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron