Hi everyone
I have just done a slump on a glass that I had sprayed Clear Coat Overglaze from Fuse Master. I used a spray gun . Now that the glass is slumped I see there is some ugly stains where the clear coat was sprayed I think this happened because the slumping took place at a 1250 F. and Clear Coat needs to go up to 1350 F. Does anyone have a suggestion on how to get rid of the stains? Should I fire the glass again at a 1350 without spraying it again or should I first spray it again and the re- fire the glass.
Thank you in advance.

Isabell
Posts: 12
Joined: Sun Oct 26, 2003 6:33 pm

Postby Isabell » Wed Oct 29, 2003 10:15 am

Hi
I have the answer to my question. I want to post it so if someone has a similar experience you can try to do this: Re-fire the glass at 1350 F.without spraying any thing else on it and the stains from the "Clear Coat Overglaze will go away.
I just got my glass out of the kiln and it looks great by just re-firing it.
I hope this will help someone sometime.
Thanks
Isabella


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 22 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com