glass needed for drop out mold

Postby Linda Hassur » Sun Nov 30, 2003 6:57 pm

I'm wanting to make a drop out mold for a serving bowl. I'm wanting to know how many layers of glass are needed for the depth of the bowl.. I think I saw this discussed but can't find it in the archives. I'm wanting it to be approx 10 inch square with a 4 inch drop. Also, what kind of firing schedule would you use. Thanks Linda

Geri Comstock
Posts: 340
Joined: Mon Mar 10, 2003 4:16 pm
Location: Northern CA
Contact:

Postby Geri Comstock » Sun Nov 30, 2003 9:36 pm

Here's a link to a discussion where drop outs are discussed.



http://www.warmglass.com/phpBB/viewtopi ... er%2A+inch


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 34 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com