2 questions, #1 about Spray A #2 problems with kiln shelf
Posted: Tue Jan 13, 2004 7:15 pm
#1 I was working with BE 0137 French Vanilla and used Spray A on it. It turned a ugly yellow color. I know that this particular glass causes problems with interactions to other glasses. I'm assuming that this is the reason I had the problem.
#2 I have a kiln shelf that has one area that won't accept kiln wash. I also have a slumper mold with the same problem. I've used sandpaper and some other methods of trying to "scuff" up the surface but these areas are "slick" and won't accept the kiln wash. I don't have a sand blaster but is there any other thing I can try? Thanks Linda
#2 I have a kiln shelf that has one area that won't accept kiln wash. I also have a slumper mold with the same problem. I've used sandpaper and some other methods of trying to "scuff" up the surface but these areas are "slick" and won't accept the kiln wash. I don't have a sand blaster but is there any other thing I can try? Thanks Linda