slumping temp for float glass
Moderators: Brad Walker, Tony Smith
-
- Posts: 44
- Joined: Sat Mar 15, 2003 10:40 pm
slumping temp for float glass
I tried to slump a very small bowl yesterday along with a couple more molds that I was using to slump. The other two completed their slumping (one with BE clear and the other float) but the small bowl never did hit the bottom of the mold. I started at 1250 and continued rising the temp in small increments until I hit 1325. I decided at this point that it wasn't going to totally slump. Any ideas? Thanks Linda
-
- Posts: 195
- Joined: Mon Mar 10, 2003 9:45 pm
- Location: SW FL
- Contact:
-
- Posts: 44
- Joined: Sat Mar 15, 2003 10:40 pm
-
- Posts: 195
- Joined: Mon Mar 10, 2003 9:45 pm
- Location: SW FL
- Contact:
-
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
I'd probably go to 1300 - 1350 depending on how fast I wanted it to happen.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions