S. Klein
Posts: 40
Joined: Tue Mar 18, 2003 8:42 pm
Location: Orange, CA

Glass paints

Postby S. Klein » Wed Jan 23, 2013 3:53 pm

I'm working with an artist in Norway. She has a large (old) supply of "Scanart" powders that she thinks might be paint. Does anyone know anything about these products? Also, "Satellite Unique" paints. Thanks
Steve Klein Studio
1650 N. Glassell, Studio U
Orange, CA 92867

Don Burt
Posts: 543
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: Glass paints

Postby Don Burt » Wed Jan 23, 2013 9:23 pm

Heres a link to a catalog from some place in Sweden that sells 'ScanArt' glass paints. See page 22
http://www.uterm.se/userimages/file/glasporslin.pdf
Satellite Unique paints were the progenitor of 'Unique Glass Colors' .
http://uniqueglasscolors.com/

It bugs me that they advertise the 'NT' version of Unique Glass Colors as nontoxic. I understand that you can probably get away with it under ACMI guidelines, but certainly the stuff has powdered glass in it if it matures at 1500F. I wouldn't let a kid use it unsupervised.

carol carson
Posts: 56
Joined: Sat Jul 30, 2005 6:25 pm
Location: Portland OR
Contact:

Re: Glass paints

Postby carol carson » Wed Jan 23, 2013 9:30 pm



Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 26 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron