troubles testing new kiln

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
mikefromitaly
Posts: 67
Joined: Thu Apr 03, 2003 7:47 am
Location: italy-sicily
Contact:

troubles testing new kiln

Post by mikefromitaly »

Hello people.

I changed fiber board on bottom of the kiln and during new tests wtih 6mm float glass i got big bubbles....
can anyone explein what it happened ? thank you in advance

mike

Image
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

http://www.picturetrail.com/mikefromitaly
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: troubles testing new kiln

Post by Bert Weiss »

The first time you fire a board, there are organics in the binders that burn out. These will stink and create gasses.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
mikefromitaly
Posts: 67
Joined: Thu Apr 03, 2003 7:47 am
Location: italy-sicily
Contact:

Re: troubles testing new kiln

Post by mikefromitaly »

thank you. so what to do ?
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

http://www.picturetrail.com/mikefromitaly
Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: troubles testing new kiln

Post by Rick Wilton »

At this point nothing, try again and it's likely resolved its self.

Once you've fired the kiln to fusing temps the organics should have all burned out and you shouldn't have any more issues. Was there smoke and a burnt sugar like smell coming out of the kiln the first time you fired with the new fibre?
Rick Wilton
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: troubles testing new kiln

Post by Bert Weiss »

Boards are not exactly flat. WIth a shelf, if there is a dip in the shelf, it can trap air which can blow that sort of bubble. There are a few solutions. You can put a piece of fiber paper beneath the glass. This will allow the air to escape. You can work on a thin sandbed. You can fill and sand the board. Or you can replace the shelf with a flatter one.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions