Failing Silicone: another option? - WarmGlass.com

Failing Silicone: another option?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
aliceRI
Posts: 39
Joined: Wed Aug 03, 2005 8:53 pm
Location: East Greenwich, RI
Contact:

Failing Silicone: another option?

Postby aliceRI » Sun Jan 12, 2014 9:41 pm

I am so frustrated. I have been using GE Silicone II for many years with only one issue about two years ago. That was from using an out-of-date tube of silicone that didn't cure. I use the silicone to adhere my glass panel to masonite or wood board. Since the summer, I have had nothing but problems. The silicone sometimes cures, sometime doesn't. I check the date, buy it at different locations, but still no consistency. I thought it might be the temperature of my studio so I have worked at keeping the pieces, after gluing, in a constant 65-70 degree environment. Still no consistency.
Does anyone use any other adhesive that is reliable for glass-to-wood applications?
HELP!

Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: Failing Silicone: another option?

Postby Greg Rawls » Mon Jan 13, 2014 8:19 am

I always buy a new tube of GE silicon II, open it and lay down a bead on a scrap. Let the bead cure for 6 hours. If it is not hard, I throw the silicon away.
Greg

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Failing Silicone: another option?

Postby rosanna gusler » Mon Jan 13, 2014 5:20 pm

ah. good idea. thanks. e 6000 works well for me
artist, owner of wanchese art studio, marine finisher


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 33 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron