Sand Mold question,

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
jim burchett
Posts: 254
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Sand Mold question,

Post by jim burchett »

I have made a Box Sand Mold and have Pressed textures into the sand to make relief in the glass. I am wondering if I sift powders into the depressed areas of the mold and then take it to a Tack fuse temp if the powders will provide contrast to those areas?
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Sand Mold question,

Post by rosanna gusler »

Probably. The Fritz might ball up before the other glass touches dowm though
artist, owner of wanchese art studio, marine finisher
jim burchett
Posts: 254
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Sand Mold question,

Post by jim burchett »

Well its worth a try...long slump at 1225 then quick up to 1400..will let you know how it works out.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie