Its been sometime since I made a plaster mold and I cant remember what all goes into it.
Can someone please give me the recipe.
Thank you,
Andrea
Image
"C'est Moi (Its Me)"
Brad Walker
Site Admin
Posts: 1489
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: making an investment

Post by Brad Walker »

The classic recipe is 1/3 plaster, 1/3 silica, 1/3 water by weight. Proportions can be close to those ratios and still work. There are lots of other recipes.

Mix dry ingredients together first, then add to water.