Hi Everyone,

Is it bad to run your kiln (110 V) when its really hot outside?

Thanks,

Tracey

Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: Kiln running when it's over 95 outside

Postby Rick Wilton » Tue Jun 30, 2015 4:29 pm

NO, it'll likely ALWAYS be 95 degrees + directly around a hot kiln anyway.
Rick Wilton

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Kiln running when it's over 95 outside

Postby Valerie Adams » Wed Jul 01, 2015 12:36 am

We hit 100° today. I ran two of my kilns simultaneously. Now and then we'll have brownouts if everyone's running their AC but hasn't happened this year.

Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Kiln running when it's over 95 outside

Postby Bert Weiss » Wed Jul 01, 2015 11:55 am

The issue with a hot environment (unless you are using solid state relays, which are heat sensitive) would be overheating the electronics in your controller. I never heard of this happening, but this forum is a great way to research this. If anybody has ever experienced this problem, let us know about it.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Kiln running when it's over 95 outside

Postby rosanna gusler » Wed Jul 01, 2015 4:41 pm

i always run a fan on my controller just because i think that it is a nice thing to do for it. r.
artist, owner of wanchese art studio, marine finisher


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 23 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com