Linda Hassur
Posts: 43
Joined: Sat Mar 15, 2003 10:40 pm

cbs frit

Postby Linda Hassur » Fri Feb 20, 2004 5:52 pm

I recently bought 7 tubes of this frit hoping that I could do a project that I had in mind. I've had lots of problems with it even though I patiently turned each piece so that the majority of the dichro was on the bottom. It balled up (dichro on dichro I guess) and I haven't been able to do anything with it except to grind off the mounds and humps on the top of the glass. I went to 1550 and held for 20 mins but I couldn't get it to smooth out. Any suggestions? Linda

Kitty
Posts: 437
Joined: Sun Mar 09, 2003 4:12 pm
Location: Gig Harbor, WA

Postby Kitty » Fri Feb 20, 2004 6:00 pm

it has to be capped.
i didnt like working with it, and wont buy it again.
for my purposes, i could cut up a bunch of tiny pieces and get a better result, without grinding and capping.

Alecia Helton
Posts: 108
Joined: Mon Aug 25, 2003 12:35 am
Location: outside of Dallas TX

Postby Alecia Helton » Fri Feb 20, 2004 6:53 pm

I've had the same problems with the Rainbow on clear. Like Kitty, I'm not sure I'll buy it again.

I've also purchased the Rainbow on black. Haven't tried it yet, but the pieces appear flatter. I' not sure it will pose the same problems.

Alecia
Alecia Helton
Wear Original Wonders!
Carrollton TX


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 44 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron