Postby mikefromitaly » Fri Oct 21, 2016 2:16 pm

Hello friends
i have a question

What is best way to polish to get shine glass ? (firepolish?cerium?spray a o borax or something else?)

thanks for support and collaboration

ciao
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

[url] http://www.picturetrail.com/mikefromitaly [/url]

Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: polishing

Postby Rick Wilton » Fri Oct 21, 2016 4:42 pm

Mike,

I don't think that can be answered at all.

It all depends on dozens of variables, thickness of glass, location of area (ie edge or face), is the glass perfectly smooth and even. thickness, shape, flat or curved etc, etc,

Good luck,

Rick
Rick Wilton

mikefromitaly
Posts: 67
Joined: Thu Apr 03, 2003 7:47 am
Location: italy-sicily
Contact:

Re: polishing

Postby mikefromitaly » Sat Feb 11, 2017 2:10 pm

Hi
thanks for reply

i meant "edge" 6mm flat glass

what do you think?

thanks

mike
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

[url] http://www.picturetrail.com/mikefromitaly [/url]

Kevin Midgley
Posts: 721
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: polishing

Postby Kevin Midgley » Sun Feb 12, 2017 1:24 am

Since you are in Italy,
http://www.bavelloni.com/

Buttercup
Posts: 571
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: polishing

Postby Buttercup » Sun Feb 12, 2017 11:52 pm

You're not doing mass production are you? Fire polish?


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 37 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com