Page 1 of 1
polishing
Posted: Fri Oct 21, 2016 2:16 pm
by mikefromitaly
Hello friends
i have a question
What is best way to polish to get shine glass ? (firepolish?cerium?spray a o borax or something else?)
thanks for support and collaboration
ciao
Re: polishing
Posted: Fri Oct 21, 2016 4:42 pm
by Rick Wilton
Mike,
I don't think that can be answered at all.
It all depends on dozens of variables, thickness of glass, location of area (ie edge or face), is the glass perfectly smooth and even. thickness, shape, flat or curved etc, etc,
Good luck,
Rick
Re: polishing
Posted: Sat Feb 11, 2017 2:10 pm
by mikefromitaly
Hi
thanks for reply
i meant "edge" 6mm flat glass
what do you think?
thanks
mike
Re: polishing
Posted: Sun Feb 12, 2017 1:24 am
by Kevin Midgley
Re: polishing
Posted: Sun Feb 12, 2017 11:52 pm
by Buttercup
You're not doing mass production are you? Fire polish?