Page 1 of 1

polishing

Posted: Fri Oct 21, 2016 2:16 pm
by mikefromitaly
Hello friends
i have a question

What is best way to polish to get shine glass ? (firepolish?cerium?spray a o borax or something else?)

thanks for support and collaboration

ciao

Re: polishing

Posted: Fri Oct 21, 2016 4:42 pm
by Rick Wilton
Mike,

I don't think that can be answered at all.

It all depends on dozens of variables, thickness of glass, location of area (ie edge or face), is the glass perfectly smooth and even. thickness, shape, flat or curved etc, etc,

Good luck,

Rick

Re: polishing

Posted: Sat Feb 11, 2017 2:10 pm
by mikefromitaly
Hi
thanks for reply

i meant "edge" 6mm flat glass

what do you think?

thanks

mike

Re: polishing

Posted: Sun Feb 12, 2017 1:24 am
by Kevin Midgley
Since you are in Italy,
http://www.bavelloni.com/

Re: polishing

Posted: Sun Feb 12, 2017 11:52 pm
by Buttercup
You're not doing mass production are you? Fire polish?